Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flex® A 8502 TPE Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Multibase
Trade Name Multi-Flex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® A 8502 TPE Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Chemical Resistance, Good Heat StabilizedOzone ResistantGeneral Purpose Moldability, GoodPaintable Forms:PelletsProcessing Method:Injection Molding Uses: Automotive Interior PartsInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
ASTM 792
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
Melt Flow 5.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
10 seconds; ASTM D2240
Tensile Strength, Yield 10.9 MPa
1580 psi
Elastic; ASTM D412
Elongation at Break 680 %
680 %
Elastic; ASTM D412
Flexural Modulus 0.0827 GPa
12.0 ksi
1% Secant; ASTM D790
Tear Strength 49.1 kN/m
280 pli
ASTM D624
Compression Set 25 %
25 %
73°F; ASTM D395
Processing Properties Metric English Comments
Middle Barrel Temperature 210 °C
410 °F
Front Barrel Temperature 227 °C
440 °F
Nozzle Temperature 235 °C
455 °F
Mold Temperature 51.7 °C
125 °F
Users viewing this material also viewed the following: