Multibase Multi-Flex® 8832 C Black TPE Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Multibase
Trade Name Multi-Flex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® 8832 C Black TPE Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.92 g/cc
1.92 g/cc
ASTM 792
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 93
93
10 seconds; ASTM D2240
Hardness, Shore D 41
41
10 seconds; ASTM D2240
Tensile Strength, Yield 5.52 MPa
800 psi
Elastic; ASTM D412
Elongation at Break 320 %
320 %
Elastic; ASTM D412
Flexural Modulus 0.310 GPa
45.0 ksi
1% Secant; ASTM D790
Tear Strength 35.1 kN/m
200 pli
ASTM D624
Thermal Properties Metric English Comments
Flame Spread 23 mm/min
0.90 in/min
FM VSS-302
Processing Properties Metric English Comments
Middle Barrel Temperature 210 °C
410 °F
Front Barrel Temperature 227 °C
440 °F
Nozzle Temperature 235 °C
455 °F
Mold Temperature 51.7 °C
125 °F