Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 5.00 - 10.0 min @Temperature 150 °C |
0.0833 - 0.167 hour @Temperature 302 °F |
|
Resinlab® EP1320 Heat Cure Epoxy Conformal Coating Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the.. |
|||
Cure Time | 5.00 - 10.0 min @Temperature 150 °C |
0.0833 - 0.167 hour @Temperature 302 °F |
|
Resinlab® EP1320LV Heat Cure Epoxy Conformal Coating Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the.. |
|||
Cure Time | 5.00 - 10.0 min @Temperature 150 °C |
0.0833 - 0.167 hour @Temperature 302 °F |
|
Resinlab® EP1325 Thixotropic, Heat Curing Epoxy Adhesive Resinlab™ EP1325 and EP1325LV are one part thixotropic, heat curing epoxy adhesives. They can also be used as a small mass potting compounds, staking or damming adhesives, or polymer systems where .. |
|||
Cure Time | 5.00 - 10.0 min @Temperature 150 °C |
0.0833 - 0.167 hour @Temperature 302 °F |
|
Resinlab® EP1325LV Thixotropic, Heat Curing Epoxy Adhesive Resinlab™ EP1325 and EP1325LV are one part thixotropic, heat curing epoxy adhesives. They can also be used as a small mass potting compounds, staking or damming adhesives, or polymer systems where .. |
|||
Cure Time | 5.00 - 10.0 min @Temperature 150 °C |
0.0833 - 0.167 hour @Temperature 302 °F |
|
Resinlab® EP1330 Heat Cure Epoxy Polymer System Resinlab™ EP1330 and EP1330LV are one part heat cure epoxy polymer systems. They can also be used as a small mass potting or staking compounds, or a dam adhesive in and “dam and fill” application.. |
|||
Cure Time | 5.00 - 10.0 min @Temperature 150 °C |
0.0833 - 0.167 hour @Temperature 302 °F |
|
Resinlab® EP1330LV Heat Cure Epoxy Polymer System Resinlab™ EP1330 and EP1330LV are one part heat cure epoxy polymer systems. They can also be used as a small mass potting or staking compounds, or a dam adhesive in and “dam and fill” application.. |
|||
Cure Time | 5.00 - 10.0 min @Temperature 120 °C |
0.0833 - 0.167 hour @Temperature 248 °F |
|
Lord Adhesives Thermosetâ„¢ MD-140 Conductive Adhesive LORD Thermosetâ„¢ MD-140 silver-filled conductive adhesive offers excellent thermal conductivity. It is designed for use in thermally demanding die attach applications such as microprocessor, po.. |
|||
Cure Time | 8.00 - 10.0 min @Temperature 100 °C |
0.133 - 0.167 hour @Temperature 212 °F |
|
Lord Adhesives Thermosetâ„¢ SC-102 Unfilled Silicone Encapsulant Lord SC-102 is a "water-white" clear, two component, silicone encapsulating system. It has a very low viscosity and, when cured, a low Shore A hardness. Lord SC-102 is optically transparent with no .. |
|||
Cure Time | 4.98 - 10.0 min @Temperature 149 °C |
0.0830 - 0.167 hour @Temperature 300 °F |
|
Master Bond Supreme 3HTND-1SM Fast Curing, One Component, Surface Mount Adhesive Master Bond Polymer System Supreme 3HTND-1SM is a one component, exceptionally fast curing surface mount adhesive system with exceptional toughness and durability. It has high shear and peel strengt.. |
|||
Cure Time | 4.98 - 10.0 min @Temperature 149 °C |
0.0830 - 0.167 hour @Temperature 300 °F |
|
Master Bond Supreme 3HTND-2GT One Part, Toughened, Fast Curing Glob Top Adhesive Master Bond Polymer System Supreme 3HTND-2GT is a fast curing, toughened one component high performance epoxy adhesive/sealant which meets the growing need for precise positioning and bonding of mic.. |
|||
Cure Time | 7.98 - 10.0 min @Temperature 75.0 °C |
0.133 - 0.167 hour @Temperature 167 °F |
Dry to handle, at 50% humidity and 75°C |
Blue River Coatings Acrylic 4000D Topcoat BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT is a hard, flexible, economical coating designed for multiple substrates. BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT offers good application properties, low fo.. |
|||
Cure Time | 7.98 - 10.0 min @Temperature 75.0 °C |
0.133 - 0.167 hour @Temperature 167 °F |
Dry to handle, at 50% humidity and 75°C |
Blue River Coatings Acrylic 4000 Topcoat BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT is a hard, flexible, economical coating designed for multiple substrates. BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT offers good application properties, low fo.. |