Blue River Coatings Acrylic 4000 Topcoat

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Blue River Coatings
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Blue River Coatings Acrylic 4000 Topcoat.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT is a hard, flexible, economical coating designed for multiple substrates. BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT offers good application properties, low foam, good adhesion, and high gloss potential. ACRYLIC 4000 TOPCOAT dries quickly (eliminating excessive grain raise on wood) and provides good sealing to help repel water. The product is designed to work in conjunction with Blue River Coatings Wood Stains and Primers.Enviromental Advantages:BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT is a low VOC (Volatile Organic Compound), performance production coating. It is considered non-hazardous by EPA definitions and does not contain lead or chromates. The solid and semi-solid sludge produced in spraying and clean up can be flocculated; dried and sent to a “Class B” landfill. Check with your local and state regulations for proper handling. Characteristics:Low cost coatingGood hardness/impact resistanceGood Solvent resistance-20 double rub MEK with little to no effectExcellent water resistance – 1 hour covered water spot test: No spotting or discolorationGood alcohol resistance –1 hour covered alcohol spot test: 50% isopropyl – slight whitening, 70% isopropyl – slight whiteningHigh solidsAvailable in satin to gloss finishCan be applied in a wide variety of temperature and humidity conditionsAir drying or force curing preferredWater is used for clean-upNon-HazardousNon-FlammableShelf life of 1 yearUsesWoodSteelAluminumSome PlasticsInformation provided by Blue River Coatings
Physical Properties Metric English Comments
Specific Gravity >= 1.00 g/cc
>= 1.00 g/cc
Density 1.03 g/cc
0.0372 lb/in³
Solids Content 39.8 %
39.8 %
by volume
45 %
45 %
by weight
Volatile Organic Compounds (VOC) Content 228 g/l
228 g/l
Thermal Properties Metric English Comments
Boiling Point 93.0 °C
199 °F
Flash Point 65.6 °C
150 °F
Processing Properties Metric English Comments
Cure Time 3.00 - 4.98 min

@Temperature 75.0 °C
0.0500 - 0.0830 hour

@Temperature 167 °F
Recoat, at 50% humidity
4.98 min

@Temperature 75.0 °C
0.0830 hour

@Temperature 167 °F
Dust Free, at 50% humidity
7.98 - 10.0 min

@Temperature 75.0 °C
0.133 - 0.167 hour

@Temperature 167 °F
Dry to handle, at 50% humidity and 75°C
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Flexibility Good
Pencil Hardness HB
Salt Spray Good
Solvent Resistance Good
Theoretical Coverage 638 ft2 at 1 mil