Processing Properties | Metric | English | Comments |
---|---|---|---|
Hold Pressure | 50.0 - 80.0 MPa | 7250 - 11600 psi | |
PolyOne Bergamid™ XP6042701 Polyamide 6 (Nylon 6) Injection Speed: 50 to 80% Holding Time: 3 to 9 sec Injection Time: 1 to 3.5 sec Cycle Time: 18 to 60 secInformation provided by PolyOne |
|||
Hold Pressure | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Akro-Plastic Akromid® S31 (3484) PA 6.10 Dry
(discontinued **) A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Hold Pressure | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Gromax PBT 4130-104D 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Hold Pressure | 40.0 - 80.0 MPa | 5800 - 11600 psi | |
Eurotec® Tecodur® PB50 NL PBT, unfilled, natural, high viscosity Information provided by Eurotec® |
|||
Hold Pressure | 40.0 - 80.0 MPa | 5800 - 11600 psi | |
Eurotec® Tecodur® PB70 GB30 NL PBT, 30% glass bead reinforced, natural Information provided by Eurotec® |
|||
Hold Pressure | 40.0 - 80.0 MPa | 5800 - 11600 psi | |
Eurotec® Tecodur® PB70 GR23 BK EF PBT, 23% glass fiber reinforced, black, suitable for electrostatic powder coating, gas injection grade Information provided by Eurotec® |
|||
Hold Pressure | 40.0 - 80.0 MPa | 5800 - 11600 psi | |
Eurotec® Tecodur® PB70 GR30 NL MB04 PBT/ASA, 30% glass fiber reinforced, heat & UV stabilized, natural Information provided by Eurotec® |
|||
Hold Pressure | 40.0 - 80.0 MPa | 5800 - 11600 psi | |
Eurotec® Tecodur® PB70 NL TD20 PBT, unfilled, flame retardant - halogen (RoHS compliant), impact modified, natural Information provided by Eurotec® |
|||
Hold Pressure | 40.0 - 80.0 MPa | 5800 - 11600 psi | |
Eurotec® Tecolen® HP10 GR30 NL HS PPCP, 30% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Hold Pressure | 40.0 - 80.0 MPa | 5800 - 11600 psi | |
Eurotec® Tecomid® NT40 GR30 NL XA60 PPA, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural Information provided by Eurotec® |
|||
Hold Pressure | 40.0 - 80.0 MPa | 5800 - 11600 psi | |
Eurotec® Tecolen® CP20 GR40 NL PPCP, 40% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Hold Pressure | 40.0 - 80.0 MPa | 5800 - 11600 psi | |
Eurotec® Tecolen® CP20 MF20 NL XA70 PPCP, 20% mineral filled, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Hold Pressure | 40.0 - 80.0 MPa | 5800 - 11600 psi | |
Eurotec® Tecomid® NT40 NL MB PPA, impact modified, heat stabilized, natural Information provided by Eurotec® |
|||
Hold Pressure | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Akro-Plastic Akroloy® PA GF 60 (2844) PA 6.6 & PA6I/6T Dry, 60% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Hold Pressure | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Akro-Plastic Akromid® T6 GF 50 (3106) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Hold Pressure | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Akro-Plastic Akromid® A3 GF 15 (2418) PA 6.6 Dry, 15% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Hold Pressure | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Dry, 35% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Hold Pressure | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Akro-Plastic Akromid® S3 GF 50 1 (3533) PA 6.10 Dry, 50% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |