Processing Properties | Metric | English | Comments |
---|---|---|---|
Hold Pressure | 30.0 - 80.0 MPa | 4350 - 11600 psi | Specific Holding Pressure |
Perstorp Compounds 136 Urea-Formaldehyde w/ cellulose filler A UF-based injection grade designed for hidden parts like sockets, circuit breakers, clamps, switches.Information provided by Perstorp Compounds Inc. |
|||
Hold Pressure | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Akro-Plastic Akromid® S31 (3484) PA 6.10 Dry
(discontinued **) A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Hold Pressure | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Gromax CCP PET 9130-104 30% Glass Filled Product Description: PET glass/mineral 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excell.. |
|||
Hold Pressure | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Gromax PBT 4130-104D 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Hold Pressure | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Gromax PBT 4130-201D 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Hold Pressure | 40.0 - 80.0 MPa | 5800 - 11600 psi | |
Eurotec® Tecodur® PB70 BK001 HS PBT, unfilled, improved impact, heat stabilized, black Information provided by Eurotec® |
|||
Hold Pressure | 40.0 - 80.0 MPa | 5800 - 11600 psi | |
Eurotec® Tecodur® PB70 GR17 BK002 FA20 PBT, 17% glass fiber reinforced, flame retardant - halogen (RoHS compliant), black Information provided by Eurotec® |
|||
Hold Pressure | 40.0 - 80.0 MPa | 5800 - 11600 psi | |
Eurotec® Tecodur® PB70 GR20 NL100 XA20 PBT, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Hold Pressure | 40.0 - 80.0 MPa | 5800 - 11600 psi | |
Eurotec® Tecolen® CP20 GB30 NL PPCP, 30% glass bead reinforced, natural Information provided by Eurotec® |
|||
Hold Pressure | 40.0 - 80.0 MPa | 5800 - 11600 psi | |
Eurotec® Tecolen® HP30 NL XC30 PPHP, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Hold Pressure | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Akro-Plastic Akromid® A3 GF 25 (2420) PA 6.6 Dry, 25% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Hold Pressure | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Dry, 35% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Hold Pressure | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Dry, 50% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Hold Pressure | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Akro-Plastic Akromid® B3 GF 20 (2470) PA 6 Dry, 20% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Hold Pressure | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Akro-Plastic Akromid® T6 GF 40 (3500) PPA Dry, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Hold Pressure | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Gromax CCP PBT 6730-104F Glass/Mineral Filled Product Description: PBT glass/mineral reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellent w.. |
|||
Hold Pressure | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Gromax PBT 3015-104 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Hold Pressure | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Gromax CCP PBT 5630-104C 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |