Lubrizol Advanced Materials Pearlthane® D91F65D Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlthane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials Pearlthane® D91F65D Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PEARLTHANE® D91F65D is an aliphatic TPU supplied in colourless natural pellets. In addition to typical TPU properties like outstanding abrasion loss, PEARLTHANE® D91F65D offers excellent colour stability upon weather exposure. This product provides high quality film and good transparency. It is especially designed for high performance extrusion and film processes.APPLICATIONS: PEARLTHANE® D91F65D is especially recommended for extrusion applications for exterior automotive parts and a variety of high performance technical parts where weather resistance and transparency are required.Information provided by Merquinsa
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Melt Flow 10 g/10 min
10 g/10 min
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
Tensile Strength, Yield 30.00 MPa
4351 psi
ASTM D412
Elongation at Break 372 %
372 %
ASTM D412
100% Modulus 0.01600 GPa
2.320 ksi
ASTM D412
300% Modulus 0.0250 GPa
3.63 ksi
ASTM D412
Abrasion 40
40
[mm^3]; DIN 53.516
Thermal Properties Metric English Comments
Melting Point 140 - 150 °C
284 - 302 °F
MQSA 114
Processing Properties Metric English Comments
Feed Temperature 155 °C
311 °F
Nozzle Temperature 170 °C
338 °F
Zone 1 170 - 180 °C
338 - 356 °F
Zone 2 180 - 190 °C
356 - 374 °F
Zone 3 190 - 200 °C
374 - 392 °F
Zone 4 185 - 195 °C
365 - 383 °F
Die Temperature 165 - 175 °C
329 - 347 °F
Mold Temperature 35.0 °C
95.0 °F
Moisture Content <= 0.10 %
<= 0.10 %
MQSA 44
Descriptive Properties Value Comments
Compression Zone 320°C
Metering Zone 320°C