Polymer Property : Zone 3 = 275 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 3 265 - 275 °C
509 - 527 °F
Lehmann & Voss LUVOCOM® 1800-8435 PET, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Zone 3 265 - 275 °C
509 - 527 °F
Lehmann & Voss LUVOCOM® 1800-8449 PET, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous d..
Zone 3 265 - 275 °C
509 - 527 °F
Lehmann & Voss LUVOCOM® 1800-7432 PET, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Zone 3 265 - 275 °C
509 - 527 °F
Lehmann & Voss LUVOCOM® 1800-7519 PET, with carbon fiber, PTFE, mineral resin
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous d..
Zone 3 265 - 275 °C
509 - 527 °F
Lehmann & Voss LUVOCOM® 1800-7806 PET, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Zone 3 230 - 275 °C
446 - 527 °F
Lehmann & Voss LUVOCOM® NY-4/PL/15/BK Polyamide 612, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Zone 3 265 - 275 °C
509 - 527 °F
Eurostar Staramide R1000K PA66, Injection Molded
Staramide R1000K is an Unreinforced Radiation Crosslinkable Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Zone 3 265 - 275 °C
509 - 527 °F
Eurostar Staramide RF004EU PA66/6, 20% Glass Fiber Filled, Injection Molded
Staramide RF004EU is a 20% Glass Fiber Reinforced Polyamide 66/6 Injection Molding (also known as Staramide 66C 20V S4)Information provided by Eurostar.
Zone 3 265 - 275 °C
509 - 527 °F
Eurostar Staramide RF006EU PA66/6, Glass Fiber Filled, Injection Molded
Staramide RF006EU is an UV stabilized, Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as Staramide 66C 30V S4)Information provided by Eurostar.
Zone 3 230 - 275 °C
446 - 527 °F
Ascend Performance Materials Vydyne® 75HF Nylon 66/6, Heat Stabilized, DAM
Vydyne® 75HF is a medium-high-viscosity, heat-stabilized PA66/6 copolymer resin designed for extrusion applications. It is available in natural color only. Vydyne 75HF resin offers a well-balanced ..