Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lehmann & Voss LUVOCOM® 1800-7806 PET, with PTFE

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1800-7806 PET, with PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.55 g/cc
1.55 g/cc
ISO 1183
Water Absorption <= 0.30 %
<= 0.30 %
23°C/24h
Linear Mold Shrinkage 0.015 - 0.020 cm/cm
0.015 - 0.020 in/in
Melt Flow <= 31 g/10 min

@Load 2.16 kg,
Temperature 250 °C
<= 31 g/10 min

@Load 4.76 lb,
Temperature 482 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
180 °C
356 °F
short term
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Insulation Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Processing Properties Metric English Comments
Processing Temperature 280 °C
536 °F
mass temp
Nozzle Temperature 265 - 275 °C
509 - 527 °F
Zone 1 285 - 295 °C
545 - 563 °F
Zone 2 270 - 280 °C
518 - 536 °F
Zone 3 265 - 275 °C
509 - 527 °F
Mold Temperature 60.0 - 120 °C
140 - 248 °F
Drying Temperature 80.0 °C

@Time 21600 - 28800 sec
176 °F

@Time 6.00 - 8.00 hour
120 °C

@Time 7200 - 18000 sec
248 °F

@Time 2.00 - 5.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color natural color (white)
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved