Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Extruded
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® LR590001 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsPETROTHENE LR590001 is designed as primary insulation for telephone singles. LR590001 is a high density resin designed for low shrinkback after extrusion. Antioxidant has been added to ensure thermal stability during processing. The resin also contains a metal deactivator to prevent degradation from copper while the cable is in service.Processing TechniquesLR590001, like other thermoplastic polyolefin resins, can be extruded as wire and cable insulation using a conventional extruder. Below are suggested extrusion conditions for LRWC409. These conditions are intended as general guidelines only, and are not optimum values, since manufacturing variables such as extruder type and size have an effect on processing of thermoplastic resins.Industry SpecificationsLR590001 meets the requirements of the following: ASTM D 1248-2, Type III, Class A, Category 4, Grades E8 and E9; Federal LP 390C, Type II, Class H, Category 4, Grade 1, REA PE-22, REA PE-39.
Physical Properties Metric English Comments
Density 0.948 g/cc
0.0342 lb/in³
ASTM D1505
ESCR 100% Igepal® 48 hour
48 hour
ASTM D1693
Melt Flow 0.80 g/10 min
0.80 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 16.2 MPa
2350 psi
ASTM D638
Tensile Strength, Yield 21.7 MPa
3150 psi
ASTM D638
Elongation at Break 590 %
590 %
ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature <= -76.1 °C
<= -105 °F
F<sub>50</sub>; ASTM D746
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
ASTM D991
Dielectric Constant 2.33

@Frequency 1.00e+6 Hz
2.33

@Frequency 1.00e+6 Hz
ASTM D1531
Dissipation Factor 0.000070

@Frequency 1.00e+6 Hz
0.000070

@Frequency 1.00e+6 Hz
ASTM D1531
Processing Properties Metric English Comments
Feed Temperature 149 - 163 °C
300 - 325 °F
Zone 2 177 - 204 °C
350 - 400 °F
Zone 3 204 - 232 °C
400 - 450 °F
Zone 4-x 246 - 260 °C
475 - 500 °F
Adapter Temperature 246 - 260 °C
475 - 500 °F
Die Temperature 246 - 260 °C
475 - 500 °F
Melt Temperature 246 - 260 °C
475 - 500 °F