Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 175 - 200 °C | 347 - 392 °F | |
Lubrizol Advanced Materials PEARLTHANE® 12K85A Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 12K85A is a standard polyester-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties. It can be e.. |
|||
Die Temperature | 175 - 200 °C | 347 - 392 °F | |
Lubrizol Advanced Materials PEARLTHANE® 12K92A Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 12K92A is a standard polyester-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties. It can be e.. |
|||
Die Temperature | 175 - 204 °C | 347 - 399 °F | Average value: 187 °C Grade Count:7 |
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum.. |
|||
Die Temperature | 175 - 200 °C | 347 - 392 °F | Extrusion |
Huntsman IROGRAN® A 70 E 4675 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 70 E 4675 is a softener free thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are very short cycle t.. |
|||
Die Temperature | 175 - 200 °C | 347 - 392 °F | Extrusion |
Huntsman IROGRAN® A 78 E 4506 TPU-Polyester Introduction: IROGRAN A 78 E 4506 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical prop.. |
|||
Die Temperature | 175 - 200 °C | 347 - 392 °F | Extrusion |
Huntsman IROGRAN® A 78 E 4723 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 78 E 4723 is a thermoplastic polyester- polyurethane for injection moulding and extrusion applications. Additional characteristics of the product are flexibility and high mec.. |
|||
Die Temperature | 175 - 205 °C | 347 - 401 °F | Extrusion |
Huntsman IROGRAN® A 85 E 4719 TPU-Polyester Introduction: IROGRAN A 85 E 4719 is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offers a.. |
|||
Die Temperature | 175 - 205 °C | 347 - 401 °F | Extrusion |
Huntsman IROGRAN® A 85 E 4993 FCM Polyester-Based TPU-Injection Extrusion Grade IROGRAN A 85 E 4993 FCM is a thermoplastic polyester polyurethane for melt calendaring. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offers a specially.. |
|||
Die Temperature | 175 - 205 °C | 347 - 401 °F | Extrusion |
Huntsman IROGRAN® A 85 E 5719 FCM TPU-Polyester Introduction: IROGRAN A 85 E 5719 FCM is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offe.. |
|||
Die Temperature | 175 - 200 °C | 347 - 392 °F | Extrusion |
Huntsman IROGRAN® A 85 H 4508 TPU-Polyester Introduction: IROGRAN A 85 H 4508 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are excellent mechanical properties and hig.. |
|||
Die Temperature | 175 - 200 °C | 347 - 392 °F | Extrusion |
Huntsman IROGRAN® A 85 P 4380 TPU-Polyether Introduction: IROGRAN A 85 P 4380 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection molding applications. Additional characteristics of th.. |
|||
Die Temperature | 175 - 200 °C | 347 - 392 °F | Extrusion |
Huntsman IROGRAN® A 85 P 4722 TPU-Polyester Introduction: IROGRAN A 85 P 4722 is a halogen-free thermoplastic- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are good microbial resista.. |
|||
Die Temperature | 175 - 205 °C | 347 - 401 °F | Extrusion |
Huntsman IROGRAN® A 85 P 5350 TPU-Polyester Introduction: IROGRAN A 85 P 5350 is a flame-retardant, halogen-free, polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 5350 is par.. |
|||
Die Temperature | 175 - 200 °C | 347 - 392 °F | Extrusion |
Huntsman IROGRAN® A 87 H 4615 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 87 H 4615 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are very short cycle times and high dimensi.. |
|||
Die Temperature | 175 - 200 °C | 347 - 392 °F | Extrusion |
Huntsman IROGRAN® A 95 H 4678 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
Die Temperature | 175 - 200 °C | 347 - 392 °F | Extrusion |
Huntsman IROGRAN® A 98 E 4066 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 98 E 4066 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are very short cycle times and high dimensi.. |
|||
Die Temperature | 175 - 215 °C | 347 - 419 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1030D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Die Temperature | 175 - 200 °C | 347 - 392 °F | Extrusion |
Huntsman IROGRAN® A 80 H 4698 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 80 H 4698 is a transparent thermoplastic polyester-polyurethane for injection molding applications. Additional characteristics of the product are good melt flow and easy demo.. |
|||
Die Temperature | 175 °C | 347 °F | Extrusion |
Huntsman IROGRAN® A 80 P 4699L Ether-Based TPU-For Cable Industry Introduction: IROGRAN A 80 P 4699 L is a high performance polyether based thermoplastic polyurethane intended for extrusion and injection mold applications. IROGRAN A 80 P 4699 L is part of the HUNT.. |
|||
Die Temperature | 175 - 200 °C | 347 - 392 °F | Extrusion |
Huntsman IROGRAN® A 88 H 4622 TPU-Polyester Introduction: IROGRAN A 88 H 4622 is a black colored thermoplastic polyether/polyester-polyurethane for injection molding and extrusion applications. Additional characteristics of the product are hi.. |
|||
Die Temperature | 175 - 200 °C | 347 - 392 °F | Extrusion |
Huntsman IROGRAN® A 92 E 4246 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 92 E 4246 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
Die Temperature | 175 - 200 °C | 347 - 392 °F | Extrusion |
Huntsman IROGRAN® A 92 E 4738 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 92 E 4738 is a white-colored, thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are flexibility and h.. |
|||
Die Temperature | 175 - 200 °C | 347 - 392 °F | Extrusion |
Huntsman IROGRAN® A 92 H 4656 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
Die Temperature | 175 - 185 °C | 347 - 365 °F | |
Lubrizol Advanced Materials PEARLCOAT® 125K Thermoplastic Polyurethane Elastomer PEARLCOAT® 125K is a polyester based TPU, supplied in form of translucent, colorless pellets, featuring medium softening point, and consistent quality pellets, low gel content as well low-tempera.. |
|||
Die Temperature | 175 - 185 °C | 347 - 365 °F | |
Lubrizol Advanced Materials PEARLCOAT® 168K Thermoplastic Polyurethane Elastomer PEARLCOAT® 168K is a polyether-based TPU, supplied in form of translucent, colorless pellets, offering adequate hardness, excellent low-temperature flexibility and very good hydrolysis resistance.. |
|||
Die Temperature | 175 - 195 °C | 347 - 383 °F | |
Lubrizol Advanced Materials PEARLCOAT® Activa D118K Thermoplastic Polyurethane Elastomer PEARLCOAT® Activa D118K is a polycaprolactone copolyester based thermoplastic polyurethane of low hardness, supplied in form of natural pellets. This product gives an inherent “low gloss asp.. |
|||
Die Temperature | 175 °C | 347 °F | 6, Extrusion |
Lubrizol Estane® ZHF 82AT0 Thermoplastic Polyurethane, Flame Retardant Type: Estane® ZHF 82AT0 NAT021 is an 82A aromatic polyether-based, non-halogen flame retardant, thermoplastic polyurethane (TPU) compound.Features: Soft, matte finished, good flame retardant proper.. |
|||
Die Temperature | 175 - 190 °C | 347 - 374 °F | |
Borealis Borstar® BB2581 HDPE for Blow Molding Borstar BB2581 is a high-density polyethylene intended for blow molding of products with high stiffness and very good environmental stress crack resistance (ESCR).Borstar BB2581 is recommended for h.. |
|||
Die Temperature | 175 - 190 °C | 347 - 374 °F | |
Borealis BS2541 High Density Polyethylene BS2541 is a high density polyethylene with very high ESCR This product is intended for blow molding. Applications: household and chemical containers such as detergents, cleaners, and motor oils, an.. |
|||
Die Temperature | 175 °C | 347 °F | Blown Film Coextrusion |
DuPont™ Appeel® 72D799 Sealing Resin DuPont™ Appeel® 72D799 is a blown or cast film resin designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDP.. |