Polymer Property : Adapter Temperature = 428 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Adapter Temperature 220 - 230 °C
428 - 446 °F
Co-extrusion with Polyamide
Petroquimica Triunfo Trithene® TN 7006 LDPE - Coextruded Film
The Trithene® TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and streng..
Adapter Temperature 220 - 230 °C
428 - 446 °F
Co-extrusion with Polyamide
Petroquimica Triunfo Trithene® TS 7006 LDPE - Coextruded Film
The Trithene TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and strength..
Adapter Temperature 220 °C
428 °F
Blow Molding
LG Chemical BM662 ABS, Heat Resistance
Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical..
Adapter Temperature 220 °C
428 °F
Blow Molding
LG Chemical BM662B ABS, Heat Resistance
Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 31621-07-5Information provided by LG Chemica..
Adapter Temperature 220 - 240 °C
428 - 464 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1055D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Adapter Temperature 220 - 240 °C
428 - 464 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1155D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical
Adapter Temperature 220 - 240 °C
428 - 464 °F
Extrusion Molding
LG Chemical KEYFLEX BT GN7155F Ester Type TPE
Description: Extrusion Molding, TPC-ET, Halogen Free Flame Retardant, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetInformation provided by LG Chemical
Adapter Temperature 220 - 260 °C
428 - 500 °F
Extrusion Molding
LG Chemical KEYFLEX BT HB9242D Ester Type TPE
Description: TPC-ET, Blow Moldable, Low Modulus, Black ColorApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5 and 1333-86-4Information provided by LG Chemical
Adapter Temperature 220 - 230 °C
428 - 446 °F
5
Lubrizol Advanced Materials Pearlthane® ECO D12T55D Thermoplastic Polyurethane
Type: Pearlthane® ECO D12T55D is a high performance bio-based thermoplastic polyurethane. With ca. 29% bio-based content.Main Application : Extrusion/MouldingSpecial Features : Properties similar..
Adapter Temperature 220 °C
428 °F
Taiwan PU Corporation TPUI-ED71 General Grade, Injection Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation.
Adapter Temperature 220 °C
428 °F
Blow Film
DuPont Appeel® LSR11D542 Lidding Sealant Resin
Appeel® LSR11D542 is a modified ethylene vinyl acetate copolymer resin designed to function as a peelable sealing layer for lidding and pouch applications. It provides a peelable seal and a "whiten..
Adapter Temperature 220 °C
428 °F
Extrusion Coating
DuPont™ Appeel® 11D888 Ethylene Vinyl Acetate
Appeel®11D888 is a developmental modified ethylene vinyl acetate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a ..