Processing Properties | Metric | English | Comments |
---|---|---|---|
Adapter Temperature | 220 - 230 °C | 428 - 446 °F | Co-extrusion with Polyamide |
Petroquimica Triunfo Trithene® TN 7006 LDPE - Coextruded Film The Trithene® TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and streng.. |
|||
Adapter Temperature | 220 - 230 °C | 428 - 446 °F | Co-extrusion with Polyamide |
Petroquimica Triunfo Trithene® TS 7006 LDPE - Coextruded Film The Trithene TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and strength.. |
|||
Adapter Temperature | 220 °C | 428 °F | Blow Molding |
LG Chemical BM662 ABS, Heat Resistance Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical.. |
|||
Adapter Temperature | 220 °C | 428 °F | Blow Molding |
LG Chemical BM662B ABS, Heat Resistance Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 31621-07-5Information provided by LG Chemica.. |
|||
Adapter Temperature | 220 - 240 °C | 428 - 464 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1055D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Adapter Temperature | 220 - 240 °C | 428 - 464 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1155D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Adapter Temperature | 220 - 240 °C | 428 - 464 °F | Extrusion Molding |
LG Chemical KEYFLEX BT GN7155F Ester Type TPE Description: Extrusion Molding, TPC-ET, Halogen Free Flame Retardant, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetInformation provided by LG Chemical |
|||
Adapter Temperature | 220 - 260 °C | 428 - 500 °F | Extrusion Molding |
LG Chemical KEYFLEX BT HB9242D Ester Type TPE Description: TPC-ET, Blow Moldable, Low Modulus, Black ColorApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5 and 1333-86-4Information provided by LG Chemical |
|||
Adapter Temperature | 220 - 230 °C | 428 - 446 °F | 5 |
Lubrizol Advanced Materials Pearlthane® ECO D12T55D Thermoplastic Polyurethane Type: Pearlthane® ECO D12T55D is a high performance bio-based thermoplastic polyurethane. With ca. 29% bio-based content.Main Application : Extrusion/MouldingSpecial Features : Properties similar.. |
|||
Adapter Temperature | 220 °C | 428 °F | |
Taiwan PU Corporation TPUI-ED71 General Grade, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
Adapter Temperature | 220 °C | 428 °F | Blow Film |
DuPont Appeel® LSR11D542 Lidding Sealant Resin Appeel® LSR11D542 is a modified ethylene vinyl acetate copolymer resin designed to function as a peelable sealing layer for lidding and pouch applications. It provides a peelable seal and a "whiten.. |
|||
Adapter Temperature | 220 °C | 428 °F | Extrusion Coating |
DuPont™ Appeel® 11D888 Ethylene Vinyl Acetate Appeel®11D888 is a developmental modified ethylene vinyl acetate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a .. |