Lubrizol Advanced Materials Pearlthane® ECO D12T55D Thermoplastic Polyurethane

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlthane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials Pearlthane® ECO D12T55D Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Pearlthane® ECO D12T55D is a high performance bio-based thermoplastic polyurethane. With ca. 29% bio-based content.Main Application : Extrusion/MouldingSpecial Features : Properties similar to standard TPU of same hardness, excellent mechanical properties and abrasion resistance.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ISO 2781
Mechanical Properties Metric English Comments
Hardness, Shore D 55
55
ISO 868
Tensile Strength 43.00 MPa
6237 psi
ISO 527-2/5A/500
Elongation at Break 360 %
360 %
ISO 527-2/5A/500
50% Modulus 0.0150 GPa
2.18 ksi
ISO 527-2/5A/500
100% Modulus 0.0180 GPa
2.61 ksi
ISO 527-2/5A/500
300% Modulus 0.0370 GPa
5.37 ksi
ISO 527-2/5A/500
Tear Strength 189 kN/m
1080 pli
Die C; ISO 527-2/5A/500
Abrasion 24
24
mm<sup>3</sup> Loss; ISO 4649-A
Thermal Properties Metric English Comments
Vicat Softening Point 133 °C
271 °F
ISO 306
Processing Properties Metric English Comments
Zone 1 200 - 210 °C
392 - 410 °F
Zone 2 205 - 215 °C
401 - 419 °F
Zone 3 210 - 220 °C
410 - 428 °F
Zone 4 215 - 225 °C
419 - 437 °F
Adapter Temperature 220 - 230 °C
428 - 446 °F
5
Die Temperature 220 - 230 °C
428 - 446 °F
6
220 - 230 °C
428 - 446 °F
TIP, 7
Dry Time 2.00 hour

@Temperature 100 °C
2.00 hour

@Temperature 212 °F
Descriptive Properties Value Comments
Biobased Content (%) 30
Compression Zone Temperature 428°F
Metering Zone Temperature 437°F