Processing Properties | Metric | English | Comments |
---|---|---|---|
Adapter Temperature | 204 - 218 °C | 400 - 425 °F | |
LyondellBasell Petrothene® GA837091 Medium Density Polyethylene
(Unverified Data**) ApplicationsPETROTHENE GA 837-091 is a broad molecular weight, medium density resin designed for use as a base resin in wire and cable jacketing. An antioxidant has been added to ensure thermal st.. |
|||
Adapter Temperature | 204 - 218 °C | 400 - 425 °F | |
LyondellBasell Petrothene® GA808091 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 808-091 is a broad molecular weight, linear low density polyethylene resin designed for use as a base resin in wire and cable jacketing. An antioxidant package is added to.. |
|||
Adapter Temperature | 204 - 218 °C | 400 - 425 °F | |
LyondellBasell Petrothene® HR92953 Medium Density Polyethylene ApplicationsPETROTHENE HR 92953 is a medium density polyethylene-based resin designed for use as jacketing for communications cable, including CATV and FOC. HR 92953 has a nominal carbon black cont.. |
|||
Adapter Temperature | 204 - 218 °C | 400 - 425 °F | |
LyondellBasell Petrothene® NA217080 Low Density Polyethylene ApplicationsPETROTHENE NA 217-080 is a natural low density polyethylene resin formulated for use as primary insulation for coaxial and control cable applications. NA 217-080 has also been designed .. |
|||
Adapter Temperature | 204 - 218 °C | 400 - 425 °F | |
LyondellBasell Petrothene® NA951080 Low Density Polyethylene ApplicationsPETROTHENE NA 951-080 is designed for use as a base resin for compounding material including gas-injected or chemically expanded insulation. NA 951-080 is a natural, low density, medium.. |
|||
Adapter Temperature | 204 - 218 °C | 400 - 425 °F | |
LyondellBasell Petrothene® PR92735 Linear Low Density Polyethylene ApplicationsPETROTHENE PR 92735 is a high molecular weight, linear low density-based compound designed for cable jacketing. PR 92735 contains a nominal carbon black content of 2.6% and antioxidant .. |
|||
Adapter Temperature | 204 °C | 399 °F | 5, Extrusion |
Lubrizol ESTANE® 58226 Ester Based Thermoplastic Polyurethane Features: Excellent physical properties, good chemical resistance and enhanced hydrolysis resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and.. |
|||
Adapter Temperature | 204 °C | 399 °F | 5, Extrusion |
Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane Features: Excellent physical and low temperature properties with very good chemical resistance and wide processing window for extrusion.Uses: Flat die/cast film and tubing extrusion and Injection an.. |
|||
Adapter Temperature | 204 - 218 °C | 399 - 424 °F | |
Clariant PEPR92735G5NAT LLDPE, 5% Glass Fiber, Chemically Coupled Data provided by Clariant Masterbatches |
|||
Adapter Temperature | 204 - 221 °C | 400 - 430 °F | Average value: 214 °C Grade Count:3 |
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and.. |
|||
Adapter Temperature | 204 - 216 °C | 399 - 421 °F | |
Lubrizol ESTANE® 58212 Ether Based Thermoplastic Polyurethane Features: Excellent clarity and UV stable with good melt strength. Pre-drying: 2 hours at 104°C (220°F) in dehumidifying hopper dryerUses: Extrusion: Cable jacket, hose/tube, profile and film and .. |
|||
Adapter Temperature | 204 °C | 399 °F | Extrusion |
Lubrizol ESTANE® 58215 Ether Based Thermoplastic Polyurethane Features: Excellent physical properties, hydrolysis resistance and improved temperature resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and b.. |