Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol ESTANE® 58212 Ether Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 58212 Ether Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Excellent clarity and UV stable with good melt strength. Pre-drying: 2 hours at 104°C (220°F) in dehumidifying hopper dryerUses: Extrusion: Cable jacket, hose/tube, profile and film and sheetInformation provided by Lubrizol.
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ASTM D2240
Hardness, Shore D 43 - 49
43 - 49
ASTM D2240
Elongation at Break 400 %
400 %
ASTM D412
100% Modulus 0.0135 GPa
1.96 ksi
ASTM D412/D638
300% Modulus 0.0316 GPa
4.58 ksi
ASTM D412/D638
Modulus of Rigidity 0.00840 GPa

@Temperature 23.0 °C
1.22 ksi

@Temperature 73.4 °F
ASTM D1053
0.0138 GPa

@Temperature 0.000 °C
2.00 ksi

@Temperature 32.0 °F
ASTM D1053
0.0413 GPa

@Temperature -20.0 °C
5.99 ksi

@Temperature -4.00 °F
ASTM D1053
0.2138 GPa

@Temperature -40.0 °C
31.01 ksi

@Temperature -40.0 °F
ASTM D1053
0.3656 GPa

@Temperature -50.0 °C
53.03 ksi

@Temperature -58.0 °F
ASTM D1053
Flexural Modulus 0.07577 GPa
10.99 ksi
ASTM D790
Tear Strength 28.9 kN/m
165 pli
Split; ASTM D470
118 kN/m
675 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 5.0
5.0
CS-17, 1000 g; ASTM D3389 B
Compression Set 36 %

@Temperature 23.0 °C,
Time 79200 sec
36 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
61 %

@Temperature 70.0 °C,
Time 79200 sec
61 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395
Tensile Set 20 %
20 %
200% elongation; ASTM D412/D638
Thermal Properties Metric English Comments
Vicat Softening Point 115 °C
239 °F
ASTM D1525
Transformation Temperature -25.0 °C
-13.0 °F
by DSC
Processing Properties Metric English Comments
Zone 1 182 - 188 °C
360 - 370 °F
Zone 2 188 - 199 °C
370 - 390 °F
Zone 3 193 - 204 °C
379 - 399 °F
Zone 4 199 - 210 °C
390 - 410 °F
Adapter Temperature 204 - 216 °C
399 - 421 °F
Die Temperature 193 - 204 °C
379 - 399 °F
Zone 2
199 - 210 °C
390 - 410 °F
Zone 1
Screw Speed 15 - 70 rpm