Processing Properties Metric English Comments
Adapter Temperature 204 - 218 °C
400 - 425 °F
LyondellBasell Petrothene® GA837091 Medium Density Polyethylene  (Unverified Data**)
ApplicationsPETROTHENE GA 837-091 is a broad molecular weight, medium density resin designed for use as a base resin in wire and cable jacketing. An antioxidant has been added to ensure thermal st..
Adapter Temperature 204 - 218 °C
400 - 425 °F
LyondellBasell Petrothene® GA808091 Linear Low Density Polyethylene
ApplicationsPETROTHENE GA 808-091 is a broad molecular weight, linear low density polyethylene resin designed for use as a base resin in wire and cable jacketing. An antioxidant package is added to..
Adapter Temperature 204 - 218 °C
400 - 425 °F
LyondellBasell Petrothene® HR92953 Medium Density Polyethylene
ApplicationsPETROTHENE HR 92953 is a medium density polyethylene-based resin designed for use as jacketing for communications cable, including CATV and FOC. HR 92953 has a nominal carbon black cont..
Adapter Temperature 204 - 218 °C
400 - 425 °F
LyondellBasell Petrothene® NA217080 Low Density Polyethylene
ApplicationsPETROTHENE NA 217-080 is a natural low density polyethylene resin formulated for use as primary insulation for coaxial and control cable applications. NA 217-080 has also been designed ..
Adapter Temperature 204 - 218 °C
400 - 425 °F
LyondellBasell Petrothene® NA951080 Low Density Polyethylene
ApplicationsPETROTHENE NA 951-080 is designed for use as a base resin for compounding material including gas-injected or chemically expanded insulation. NA 951-080 is a natural, low density, medium..
Adapter Temperature 204 - 218 °C
400 - 425 °F
LyondellBasell Petrothene® PR92735 Linear Low Density Polyethylene
ApplicationsPETROTHENE PR 92735 is a high molecular weight, linear low density-based compound designed for cable jacketing. PR 92735 contains a nominal carbon black content of 2.6% and antioxidant ..
Adapter Temperature 204 - 221 °C
400 - 430 °F
Average value: 214 °C Grade Count:3
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and..