Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol ESTANE® 58226 Ester Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 58226 Ester Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Excellent physical properties, good chemical resistance and enhanced hydrolysis resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provide by Lubrizol.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Maximum Moisture Content 0.020
0.020
Mechanical Properties Metric English Comments
Hardness, Shore A 89 - 95

@Time 5.00 sec
89 - 95

@Time 0.00139 hour
ASTM D2240
Tensile Strength 58.99 MPa
8556 psi
28 days immersion in Diesel Fuel
60.85 MPa
8826 psi
15 days immersion in Diesel Fuel
62.1 MPa
9010 psi
ASTM D412
Elongation at Break 500 %
500 %
ASTM D412/D638
100% Modulus 0.00760 GPa
1.10 ksi
ASTM D412
300% Modulus 0.0207 GPa
3.00 ksi
ASTM D412
Tear Strength 26.3 kN/m
150 pli
Trouser; ASTM D470
Graves Tear Strength 99.9 kN/m
570 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 40
40
H18, 1000g; ASTM D3389
Tensile Set 21 %
21 %
200% elongation; ASTM D412
Thermal Properties Metric English Comments
Melting Point 140 °C
284 °F
DSC
Vicat Softening Point 83.9 °C
183 °F
ASTM D1525
Glass Transition Temp, Tg -25.0 °C
-13.0 °F
DSC
Processing Properties Metric English Comments
Zone 1 182 °C
360 °F
Extrusion
Zone 2 188 °C
370 °F
Extrusion
Zone 3 193 °C
379 °F
Extrusion
Zone 4 199 °C
390 °F
Extrusion
Adapter Temperature 204 °C
399 °F
5, Extrusion
Die Temperature 204 °C
399 °F
Zone 1, 6, Extrusion
204 °C
399 °F
Zone 2, Extrusion
Drying Temperature 104 °C
219 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Dew Point -40.0 °C
-40.0 °F
Descriptive Properties Value Comments
Volume swell in Diesel Fuel 8%
24 hr, ASTM D471