Polymer Property : Pot Life = 600 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Pot Life 1.50 - 600 min
1.50 - 600 min
Average value: 41.7 min Grade Count:59
Overview of materials for Thermoset Polyurethane, Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values ..
Pot Life 480 - 600 min

@Temperature 25.0 °C
480 - 600 min

@Temperature 77.0 °F
Cytec Conathane® CC-1155-35 (Conap) Polyurethane Two-component Dielectric Conformal Coating
Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i..