Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 1.50 - 600 min | 1.50 - 600 min | Average value: 41.7 min Grade Count:59 |
Overview of materials for Thermoset Polyurethane, Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values .. |