Processing Properties Metric English Comments
Injection Pressure 2.41 - 8.27 MPa
350 - 1200 psi
Multibase Nylex™ 1230 Natural Polyamide + PP
Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Methods:Injection MoldingUses: Electrical PartsHousing..
Injection Pressure 2.41 - 8.27 MPa
350 - 1200 psi
Multibase Nylex™ 1404 NAT Polyamide + PP
Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Methods:Injection MoldingUses: Electrical PartsHousing..
Injection Pressure 2.41 - 8.27 MPa
350 - 1200 psi
Multibase Nylex™ 2185 NAT Polyamide + PP
Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Methods:Injection MoldingUses: Electrical PartsHousing..
Injection Pressure 2.41 - 8.27 MPa
350 - 1200 psi
Multibase Nylex™ 2185 R15 Polyamide + PP
Glass fiber reinforcement, 15% Filler by Weight. Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Metho..
Injection Pressure 2.41 - 8.27 MPa
350 - 1200 psi
Multibase Nylex™ 2185 R30 Polyamide + PP
Glass fiber reinforcement, 30% Filler by Weight Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Method..
Injection Pressure 2.41 - 8.27 MPa
350 - 1200 psi
Multibase Nylex™ 2185 FR Polyamide + PP
Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodFlame RetardantForms:PelletsProcessing Methods:Injection MoldingUses: Electric..