Material Notes:
Data provided by Clariant Masterbatches
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.015 cm/cm
0.015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 57.2 MPa
8300 psi
ASTM D638
Flexural Yield Strength 103 MPa
15000 psi
ASTM D790
Flexural Modulus 2.55 GPa
370 ksi
ASTM D790
Izod Impact, Notched 1.87 J/cm

@Temperature 22.8 °C
3.50 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 82.2 °C
180 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 232 - 260 °C
450 - 500 °F
Mold Temperature 51.7 - 79.4 °C
125 - 175 °F
Dry Time 2 - 4 hour

@Temperature 104 °C
2 - 4 hour

@Temperature 220 °F
to ensure moisture content is less than 0.2%
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
8.27 - 13.8 MPa
1200 - 2000 psi
Initial
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Shot Size 30 - 80 %
30 - 80 %
Screw Speed 20 - 100 rpm
20 - 100 rpm