Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 35.0 - 100 MPa | 5080 - 14500 psi | |
Zhejiang Juner PA66-301-G0 Flame-Retardant & Glass Reinforced, Non-Halogen PA66 Applications: Electric Appliance PedestalInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Injection Pressure | 35.0 - 125 MPa | 5080 - 18100 psi | |
BASF Ultramid® 8200 HS PA 6 (Conditioned) Description: Ultramid 8200 HS is a heat stabilized, medium viscosity, PA6 injection molding homopolymer, exhibiting resistance to sink-mark formation in thick sections, and improved toughness over c.. |
|||
Injection Pressure | 35.0 - 125 MPa | 5080 - 18100 psi | |
BASF Ultramid® 8200 HS PA 6 (Dry) Description: Ultramid 8200 HS is a heat stabilized, medium viscosity, PA6 injection molding homopolymer, exhibiting resistance to sink-mark formation in thick sections, and improved toughness over c.. |
|||
Injection Pressure | 35.0 - 125 MPa | 5080 - 18100 psi | |
BASF Ultramid® 82335G HS BK 102 50% Glass Filled PA6 (Conditioned) Description: Ultramid 8235G HS BK-102 is a heat stabilized, pigmented black, 50% glass fiber reinforced PA6 injection molding compound offering excellent level of strength, stiffness, high temperatu.. |
|||
Injection Pressure | 35.0 - 125 MPa | 5080 - 18100 psi | |
BASF Ultramid® 82335G HS BK 102 50% Glass Filled PA6 (Dry) Description: Ultramid 8235G HS BK-102 is a heat stabilized, pigmented black, 50% glass fiber reinforced PA6 injection molding compound offering excellent level of strength, stiffness, high temperatu.. |
|||
Injection Pressure | 35.0 - 125 MPa | 5080 - 18100 psi | |
BASF Ultramid® B3WGM24 HPX BK 2320 30% Glass/Mineral Filled PA6 (Dry) Description: Ultramid B3WGM24 HPX BK23210 is a very high productivity, 30% glass/mineral reinforced heat stabilized injection molding PA6 grade for components that require medium rigidity, excellent.. |
|||
Injection Pressure | 35.0 - 125 MPa | 5080 - 18100 psi | |
BASF Ultramid® N-276 BK ND 3007 40% Glass/Mineral Filled PA66 Description: Ultramid N-276 BK ND3007 is a 40% mineral/glass reinforced, heat stabilized injection molding PA6/6.Information provided by BASF |
|||
Injection Pressure | 35.0 - 125 MPa | 5080 - 18100 psi | |
BASF Ultramid® 1503-2F BK ND 3007 33% Glass Filled PA 66 (Conditioned) Description: Ultramid 1503-2F BK ND3007 is a 33% glass reinforced, heat stabilized injection molding PA6/6 grade. It is designed to provide enhance hydroysis resistance for under-the-hood applicatio.. |
|||
Injection Pressure | 35.0 - 125 MPa | 5080 - 18100 psi | |
BASF Ultramid® 1503-2F BK ND 3007 33% Glass Filled PA 66 (Dry) Description: Ultramid 1503-2F BK ND3007 is a 33% glass reinforced, heat stabilized injection molding PA6/6 grade. It is designed to provide enhance hydroysis resistance for under-the-hood applicatio.. |
|||
Injection Pressure | 35.0 - 125 MPa | 5080 - 18100 psi | |
BASF Ultramid® AZ HP UV BK 23220 PA66 (Dry) Description: Ultramid A3Z HP UV BK23220 is an impact modified PA66 containing heat and ultraviolet light stabilizers. Designed for maximum toughness at low temperatures, Ultramid A3Z HP UV BK23220 o.. |