Material Notes:
Description: Ultramid A3Z HP UV BK23220 is an impact modified PA66 containing heat and ultraviolet light stabilizers. Designed for maximum toughness at low temperatures, Ultramid A3Z HP UV BK23220 offers a unique combination of impact performance and excellent processability.Information provided by BASF
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 46.0 MPa
6670 psi
ISO 527
Elongation at Break 50 %
50 %
Nominal; ISO 527
Flexural Modulus 1.703 GPa
247.0 ksi
ISO 178
Izod Impact, Notched (ISO) 22.0 kJ/m²

@Temperature -40.0 °C
10.5 ft-lb/in²

@Temperature -40.0 °F
ISO 180
83.0 kJ/m²

@Temperature 23.0 °C
39.5 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Melting Point 258 °C
496 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C
145 °F
ISO 75
Processing Properties Metric English Comments
Melt Temperature 280 - 304 °C
536 - 579 °F
Mold Temperature 60.0 - 100 °C
140 - 212 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 2 - 4 hour
2 - 4 hour
Moisture Content >= 0.20 %
>= 0.20 %
Injection Pressure 35.0 - 125 MPa
5080 - 18100 psi
Back Pressure 0.000 - 0.350 MPa
0.000 - 50.8 psi
Screw Speed 40 - 80 rpm
40 - 80 rpm