BASF Ultramid® 8200 HS PA 6 (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer BASF
Trade Name Ultramid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® 8200 HS PA 6 (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Ultramid 8200 HS is a heat stabilized, medium viscosity, PA6 injection molding homopolymer, exhibiting resistance to sink-mark formation in thick sections, and improved toughness over conventional lower viscosity grades. It possesses a combination of strength, stiffness and toughness properties as well as excellent heat, chemical and abrasion resistance. It is available in natural and pigmented versions.Applications: Ultramid 8200 HS is generally recommended for application such as wiring devices, plugs, receptacles, gears, connectors, convoluted tubing, filter housings, hinges, and textile components.Information provided by BASF
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 1.6 %
1.6 %
24 Hours; ISO 62
2.7 %
2.7 %
50% RH; ISO 62
9.5 %
9.5 %
Saturation; ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Yield 39.0 MPa
5660 psi
23; ISO 527
120 MPa

@Temperature -40.0 °C
17400 psi

@Temperature -40.0 °F
ISO 527
Elongation at Break >= 50 %
>= 50 %
ISO 527
Elongation at Yield 16 %
16 %
ISO 527
Processing Properties Metric English Comments
Melt Temperature 240 - 285 °C
464 - 545 °F
Mold Temperature 65.0 - 80.0 °C
149 - 176 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 2 - 4 hour
2 - 4 hour
Moisture Content >= 0.15 %
>= 0.15 %
Injection Pressure 35.0 - 125 MPa
5080 - 18100 psi
Descriptive Properties Value Comments
Commercial Status North America