Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 2.76 - 8.27 MPa | 400 - 1200 psi | |
RheTech Products FRG130-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Flame Retardant, Black Applications: Electrical component housingsSunroof componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 8.27 MPa | 400 - 1200 psi | |
RheTech Products FRP102-01 Polypropylene, Flame Retardant, Black Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 8.27 MPa | 400 - 1200 psi | |
RheTech Products FRP300-00 20% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Natural Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant 612-01 HSL Black Nylon 612, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant PBTSP0008WT-199 Polybutylene Terephthalate, Glass Reinforced, Flame Retardant Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol 612G10-L Nylon 612, 10% Glass Fiber Reinforced, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol 6253 Nylon 6, High Impact Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol 6601FR Nylon 66, Flame Retardant Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol ABS3470 ABS, High Heat, Low Gloss Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol BR4014BK ABS, High Gloss, Black Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA113G13 Nylon 66, 13% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA113G13X050 Nylon 66, 13% Glass Fiber, Heat Stabilized, Lubricated, Improved Ductility Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA123 Nylon 66, Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA123G13 Nylon 66, 13% Glass Fiber, Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA213 Nylon 6, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA213G30 Nylon 6, 30% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA223G13 Nylon 6, 13% Glass Fiber, Impact Modified Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA233G13HT Nylon 6, 13% Glass Fiber, Improved Processability, Easily Colorable, Highly Toughened Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA2SP0006 Nylon 6, Heavyweight Compound Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA2SP0011HW Nylon 6, Heavyweight Compound Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA2SP0024 Nylon 6, Flame Retardant, Static Dissipative Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PCSP0006WT-181 Polycarbonate, Laser Markable Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PCSP0015 Polycarbonate, Carbon Fiber Filled Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PCSP0016BL-201 Polycarbonate/Polyester Alloy Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PP1100G40 Polypropylene Homopolymer, 40% Glass Fiber, Chemically Coupled Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol R66G13HSL Nylon 66, 13% Glass Fiber, Heat Stabilized, Lubricated, Economy Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA111BK S&P Nylon 66, General Purpose Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA111G33 Nylon 66, 33% Glass Fiber Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PPSP0005 Polypropylene Homopolymer, Glass Fiber and Mica Reinforced, Chemically Coupled Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol 66G33-L Nylon 66, 33% Glass Fiber Reinforced, Lubricated Data provided by Clariant Masterbatches |