Aremco Corr-Paint™ CP4070 High Temperature Protective Coating Silicone, Aluminum Filled

Category Other Engineering Material , Ceramic/Metallic Coating , Polymer , Thermoset , Silicone
Manufacturer Aremco
Trade Name Corr-Paint™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Corr-Paint™ CP4070 High Temperature Protective Coating Silicone, Aluminum Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, and offer outstanding resistance to outdoor weathering, UV light, salt spray, chemical corrosion, thermal cycling, and temperatures to 1100 ºF.
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
Solids Content 38.5 %
38.5 %
by volume
44.8 %
44.8 %
by weight
Volatile Organic Compounds (VOC) Content 121 g/l
121 g/l
Viscosity 300 - 600 cP
300 - 600 cP
Thickness 25.4 microns
1.00 mil
recommended dry film thickness
66.0 microns
2.60 mil
estimated wet film thickness
Storage Temperature 12.8 - 29.4 °C
55.0 - 85.0 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 593 °C
1100 °F
Flash Point >= 100 °C
>= 212 °F
Processing Properties Metric English Comments
Processing Temperature 10.0 - 48.9 °C
50.0 - 120 °F
Application Temperature
Dry Time 1.00 - 2.00 hour
1.00 - 2.00 hour
Touch
2.00 - 4.00 hour
2.00 - 4.00 hour
Handling
1.0 - 24.0 hour
1.0 - 24.0 hour
Recoat
Cure Time >= 60.0 min
>= 1.00 hour
Air Set prior to curing
45.0 min

@Temperature 249 °C
0.750 hour

@Temperature 480 °F
60.0 min

@Temperature 232 °C
1.00 hour

@Temperature 450 °F
Adequate ventilation is required when curing these products. Outgassing will occur above 300°F and cease after 750°F. An additional 30 minutes is required at the highest service temperature if service temperature is below 750°F.
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Color Blue
Dry Film Coverage ft2/gal 617
at 1 mil
Primer Not Required
Thinner Water
Users viewing this material also viewed the following: