Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 200 - 235 °C | 392 - 455 °F | Barrel Temperature |
SABIC PP 412MK49 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 412MK49 is specially developed for producing injection molded articles. This grade contains an antistatic & nucleating agents. It has medium flow properties, good impact r.. |
|||
Processing Temperature | 200 - 235 °C | 392 - 455 °F | Barrel Temperature |
SABIC PP 413MNK45 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 413MNK45 is a controlled rheology PP grade with a very high fluidity. It is provided with an antistatic package & nucleating agent and is especially developed for producing.. |
|||
Processing Temperature | 220 - 235 °C | 428 - 455 °F | Barrel Temperature |
SABIC PP 513MN40 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 513MN40 is a controlled rheology PP grade of narrow molecular weight distribution. It contains an antistatic agent and is especially developed for producing injection molde.. |
|||
Processing Temperature | 200 - 235 °C | 392 - 455 °F | Barrel Temperature |
SABIC PP 5707N Polypropylene Homopolymer STIFFPACT for Injection Molding Product Description: PP 5707N is a reactor PP homopolymer grade with antistatic and nucleated agents. It is suitable for producing injection molded applications and gives consistent processability.. |
|||
Processing Temperature | 210 - 235 °C | 410 - 455 °F | Barrel Temperature |
SABIC PP 578P Polypropylene Homopolymer for Injection Molding Product Description: PP 578P is a controlled rheology PP grade of medium molecular weight distribution suitable for injection molding applications. It gives consistent processability, good flow pr.. |
|||
Processing Temperature | 230 - 235 °C | 446 - 455 °F | Reflow Soldering (Peak) |
Nihon Superior SN96Cl Lead-Free Solder Alloy |
|||
Processing Temperature | 160 - 235 °C | 320 - 455 °F | Average value: 221 °C Grade Count:9 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade". Each property range of values reported.. |
|||
Processing Temperature | 215 - 235 °C | 419 - 455 °F | hot runner |
Celanese RITEFLEX 663 TPC, Unfilled Riteflex 663 is a nominal 63 Shore D thermoplastic polyester elastomer with medium modulus.Information provided by Celanese |
|||
Processing Temperature | 205 - 235 °C | 401 - 455 °F | hot runner |
Celanese RITEFLEX 655A TPC, Unfilled Riteflex 655A is a thermoplastic polyester elastomer with nominal shore D hardness of 55 and medium modulus.Information provided by Celanese |
|||
Processing Temperature | 205 - 235 °C | 401 - 455 °F | hot runner |
Celanese RITEFLEX 655HS TPC, Unfilled 55 Shore D Hardness heat stabilizedInformation provided by Celanese |
|||
Processing Temperature | 220 - 235 °C | 428 - 455 °F | hot runner |
Celanese RITEFLEX 672 TPC, Unfilled Riteflex 672 is a 72 Shore D Hardness thermoplastic polyester elastomer with a high modulus.Information provided by Celanese |