Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 618.3 - 732 °C | 1145 - 1350 °F | Brazing Range |
Lucas-Milhaupt EASY FLO 45 Silver Based Cadmium-Bearing Filler Metal Applications: Easy-Flo 45 is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wet.. |
|||
Processing Temperature | 618.3 - 760 °C | 1145 - 1400 °F | Brazing Temperature |
Lucas-Milhaupt Silvally® 45 Flux Coated Rod Brazing Alloy Silvaloy 45 FC is the lowest melting brazing alloy available composed of silver, copper, zinc, and cadmium. It is suitable for use on most metals except aluminum and magnesium. It is used for joinin.. |
|||
Processing Temperature | 618.3 - 760 °C | 1145 - 1400 °F | Brazing Temperature |
Lucas-Milhaupt Silvaloy® 45 Brazing Alloy Silvaloy 45 is the lowest melting brazing alloy available composed of silver, copper, zinc, and cadmium. It is suitable for use on most metals except aluminum and magnesium. It is used for joining s.. |