Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 690 °C | 1270 °F | Typical Firing Temperature; Typical Firing Time: 5-10 min. |
Ferro IX 2683 Passivation Glasses - High Voltage (Zn-B-Silicates) Typical Powder Form: DSD Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures and ca.. |
|||
Processing Temperature | 688 - 788 °C | 1270 - 1450 °F | Brazing Range |
Lucas-Milhaupt FOS FLO 670 Copper Phosphorus Tin Braze Filler Metal Applications:Fos-Flo 7 iFos-Flo 670 is a low cost brazing filler metal suitable for joining copper to copper and copper to copper alloys where critical impact or vibration stresses are not encounter.. |
|||
Processing Temperature | 690 °C | 1270 °F | Typical Firing Temperature; Typical Firing Time: 10-15 min. at Peak |
Ferro IP 745 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Processing Temperature | 688 - 760 °C | 1270 - 1400 °F | Brazing Range |
Lucas-Milhaupt EASY FLO 3 Carbide Brazing Alloy Easy-Flo 3 is recommended for use on stainless steels subject to chloride corrosion, such as marine hardware, fishing tackle, and some dairy equipment cleaned with bleaching solutions and other equi.. |
|||
Processing Temperature | 688 - 816 °C | 1270 - 1500 °F | Brazing Temperature |
Lucas-Milhaupt Silvaloy® 50N Brazing Alloy Silvaloy 50N is a modification of Silvaloy 50. It was originally introduced because of somewhat better corrosion resistance than Silvaloy 50 for certain conditions, and is still used for such purpos.. |