Lucas-Milhaupt Silvaloy® A56T Brazing Alloy

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy , Solder/Braze Alloy
Manufacturer Lucas-Milhaupt
Trade Name Silvaloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucas-Milhaupt Silvaloy® A56T Brazing Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Silvaloy A56T has the lowest brazing temperature, best wetting, and best flow of all the cadmium free alloys. It has a slight plastic range which may be noticed during melting on some applications. Its low zinc content minimizes problems due to longer heating cycles or due to excessive heating. It is often selected for use on silver or stainless steel due to its excellent color match. Typical applications are the joining of ferrous, non-ferrous, and dissimilar metals and alloys with close joint clearances.Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).
Physical Properties Metric English Comments
Specific Gravity 9.49 g/cc
9.49 g/cc
Density 9.492 g/cc
0.3429 lb/in³
Thermal Properties Metric English Comments
Melting Point 618.3 - 651.7 °C
1145 - 1205 °F
Solidus 618.3 °C
1145 °F
Liquidus 651.7 °C
1205 °F
Maximum Service Temperature, Air 204 °C
400 °F
continuous
316 °C
600 °F
intermittent
Component Elements Properties Metric English Comments
Copper, Cu 21 - 23 %
21 - 23 %
Other, total <= 0.15 %
<= 0.15 %
Silver, Ag 55 - 57 %
55 - 57 %
Tin, Sn 4.5 - 5.5 %
4.5 - 5.5 %
Zinc, Zn 15 - 19 %
15 - 19 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000145 ohm-cm
0.0000145 ohm-cm
Processing Properties Metric English Comments
Processing Temperature 651.7 - 760 °C
1205 - 1400 °F
Brazing Temperature
Descriptive Properties Value Comments
Color White
Electrical Conductivity (% IACS) 11.9