Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 100 - 200 °C |
66.7 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA)
(Unverified Data**) Amodel AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temper.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 100 - 200 °C |
66.7 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 100 - 200 °C |
66.7 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin. Th.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® FG400MTD BLA079 Acetal
(Unverified Data**) Delrin® FG400MTD BLA079 is a metal filled, medium viscosity acetal copolymer for injection molding. It is detected in metal detectors. It has been developed for consideration into applications such.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500AL is a medium viscosity acetal homopolymer, lubricated for low wear and /or coefficient of friction. It has been developed for consideration into applications such as parts for the fo.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6
(Unverified Data**) Zytel® 73G30T NC010 is a 30% glass fiber reinforced, toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6
(Unverified Data**) Zytel® 73G30T NC010 is a 30% glass fiber reinforced, toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612
(Unverified Data**) Zytel® 151 NC010 is a PA 612 resin.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
|
Aardvark Polymers AARTEL® 2100UV Acetal Homopolymer Rotational Molding Resin Aartel 2100UV is a natural acetal homopolymer with UV stabilizers.Aartel 2100UV is a medium viscosity resin with excellent flow characteristics.Aartel 2100UV is available in natural white and may be.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 60.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl RF1132 PPE+PP PPE+PP blend for high frequency applications. Good heat resistance and low DK.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature -30.0 - 80.0 °C |
66.7 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL ZX09022 PPE+PP (Europe-Africa-Middle East) Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 100 - 200 °C |
66.7 µin/in-°F @Temperature 212 - 392 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® A-4133 HH Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-4133 HH is a 33% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation .. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 100 - 200 °C |
66.7 µin/in-°F @Temperature 212 - 392 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® A-4145 HH Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® A-4145 HH is a 45% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation .. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 100 - 200 °C |
66.7 µin/in-°F @Temperature 212 - 392 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samp.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 100 - 250 °C |
66.7 µin/in-°F @Temperature 212 - 482 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications .. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 100 - 200 °C |
66.7 µin/in-°F @Temperature 212 - 392 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Dry) Amodel® AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 150 - 200 °C |
66.7 µin/in-°F @Temperature 302 - 392 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Lavanta® 5115 WH224 Polyester, High Performance (HPP), 15% Glass Fiber Lavanta® 5115 WH224 is a 15% glass fiber reinforced, high-performance polyester (HPP) injection molding grade developed specifically for HB LED packaging applications that utilize surface mount t.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature -40.0 - 40.0 °C |
66.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 420HP PBT 30% Glass filled PBT resin, FDA Food Contact compliant in limited colors. Effective March 2008 this grade will no longer be supported with biocompatibility information. Alternative grade Valox HX420.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature -40.0 - 40.0 °C |
66.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® V2105U PBT Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature -50.0 - 50.0 °C |
66.7 µin/in-°F @Temperature -58.0 - 122 °F |
ISO 11359-2 |
Chevron Phillips Xtel® XE3035BL Polyphenylene Sulfide Alloy Xtel® XE3035BL is a high performance, glass fiber reinforced, PPS based alloy developed to provide exceptionally high ductility and impact resistance along with good thermal stability.Information p.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 100 - 200 °C |
66.7 µin/in-°F @Temperature 212 - 392 °F |
ISO 11359-2 |
Chevron Phillips Xtel® XE3035BL Polyphenylene Sulfide Alloy Xtel® XE3035BL is a high performance, glass fiber reinforced, PPS based alloy developed to provide exceptionally high ductility and impact resistance along with good thermal stability.Information p.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature -50.0 - 50.0 °C |
66.7 µin/in-°F @Temperature -58.0 - 122 °F |
ISO 11359-2 |
Chevron Phillips Xtel® XE3035NA Polyphenylene Sulfide Alloy Xtel® XE3035NA is a high performance, glass fiber reinforced, PPS based alloy developed to provide exceptionally high ductility and impact resistance along with good thermal stability.Information p.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 100 - 200 °C |
66.7 µin/in-°F @Temperature 212 - 392 °F |
ISO 11359-2 |
Chevron Phillips Xtel® XE3035NA Polyphenylene Sulfide Alloy Xtel® XE3035NA is a high performance, glass fiber reinforced, PPS based alloy developed to provide exceptionally high ductility and impact resistance along with good thermal stability.Information p.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® ST801AHS NC010 Nylon 66
(Unverified Data**) Zytel® ST801AHS NC010 is a Super Tough, high performance polyamide 66 resin. It offers outstanding molding performance in injection molding applications.Information provided by DuPont |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® ST801AW NC010 Nylon 66
(Unverified Data**) Zytel® ST801AW NC010 is a Super Tough, high performance polyamide 66 resin. It is UV stabilized and when appropriately colored offers the best resistance to indirect sunlight in automotive interior.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 160 - 250 °C |
66.7 µin/in-°F @Temperature 320 - 482 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G30NHF BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin with improved flow. It is also a PPA resin and it uses a non-halogenated flame ret.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 100 - 200 °C |
66.7 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
Solvay Specialty Polymers Amodel® A-1240 L Polyphthalamide (PPA)
(discontinued **) Amodel A-1240 L is a 40% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 149 - 249 °C |
66.7 µin/in-°F @Temperature 300 - 480 °F |
ASTM E831 |
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications incl.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 149 - 249 °C |
66.7 µin/in-°F @Temperature 300 - 480 °F |
ASTM E831 |
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 55.0 - 160 °C |
66.7 µin/in-°F @Temperature 131 - 320 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)