Chevron Phillips Xtel® XE3035BL Polyphenylene Sulfide Alloy

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer Chevron Phillips Chemical Company LP
Trade Name Xtel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Xtel® XE3035BL Polyphenylene Sulfide Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Xtel® XE3035BL is a high performance, glass fiber reinforced, PPS based alloy developed to provide exceptionally high ductility and impact resistance along with good thermal stability.Information provided by Chevron PhillipsMeasured on 102mm x 102mm x 3.2 mm plaques, edge gated.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183A
Water Absorption 0.10 %
0.10 %
ASTM D-570
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 100 MPa
14500 psi
ISO 527
Elongation at Yield 2.5 %
2.5 %
ISO 527
Flexural Strength 140 MPa
20300 psi
ISO 178
Flexural Modulus 7.50 GPa
1090 ksi
ISO 178
Compressive Strength 90.0 MPa
13100 psi
ISO 604
Izod Impact, Notched (ISO) 15.0 kJ/m²
7.14 ft-lb/in²
ISO 180A
Izod Impact, Unnotched (ISO) 40.0 kJ/m²
19.0 ft-lb/in²
ISO 180A
Thermal Properties Metric English Comments
CTE, linear 10.0 µm/m-°C

@Temperature 100 - 200 °C
5.56 µin/in-°F

@Temperature 212 - 392 °F
Axial; ISO 11359-2
20.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
11.1 µin/in-°F

@Temperature -58.0 - 122 °F
Axial; ISO 11359-2
CTE, linear, Transverse to Flow 120 µm/m-°C

@Temperature -50.0 - 50.0 °C
66.7 µin/in-°F

@Temperature -58.0 - 122 °F
ISO 11359-2
120 µm/m-°C

@Temperature 100 - 200 °C
66.7 µin/in-°F

@Temperature 212 - 392 °F
ISO 11359-2
Thermal Conductivity 0.280 W/m-K
1.94 BTU-in/hr-ft²-°F
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
ISO 75
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D-257
Insulation Resistance 1.00e+10 ohm

@Temperature 90.0 °C,
Time 173000 sec
1.00e+10 ohm

@Temperature 194 °F,
Time 48.0 hour
95% RH
Dielectric Constant 3.5

@Frequency 1000 Hz
3.5

@Frequency 1000 Hz
ASTM D-150
3.5

@Frequency 1e+6 Hz
3.5

@Frequency 1e+6 Hz
ASTM D-150
Dielectric Strength 20.0 kV/mm
508 kV/in
ASTM D-149
Dissipation Factor 0.0010

@Frequency 1000 Hz
0.0010

@Frequency 1000 Hz
ASTM D-150
0.011

@Frequency 1e+6 Hz
0.011

@Frequency 1e+6 Hz
ASTM D-150
Arc Resistance 120 sec
120 sec
ASTM D-495
Comparative Tracking Index 150 V
150 V
UL 746A
Processing Properties Metric English Comments
Melt Temperature 315 - 345 °C
599 - 653 °F
Mold Temperature 135 °C
275 °F
Users viewing this material also viewed the following: