Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Parallel to Flow = 74.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 74.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
41.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® LUX9130T PC COPOLYMER (Asia Pacific)
LUX9130T Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm / 5VA rating at 6.0mm and is U..
CTE, linear, Parallel to Flow 74.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP DL001 PC
LNP* LUBRICOMP* DL001 is a compound based on Polycarbonate resin containing 5% PTFE. Added features of this material include: Internally Lubricated.
CTE, linear, Parallel to Flow 74.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP DL001 PC (Asia Pacific)
LNP* Lubricomp* DL001 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated.
CTE, linear, Parallel to Flow 74.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Lubricomp CI001 PS
LNP* Lubricomp* CI001 is a compound based on Polystyrene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the America..
CTE, linear, Parallel to Flow 74.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP DL003E PC (Asia Pacific)
LNP LUBRICOMP* DL003E is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Easy Molding.
CTE, linear, Parallel to Flow 74.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP DL003EU PC
LNP LUBRICOMP* DL003EU is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Easy Molding, UV Stabilized, Internally Lubricated.
CTE, linear, Parallel to Flow 74.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Noryl V01505 PPE+HIPS
Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
CTE, linear, Parallel to Flow 74.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Noryl V01505 PPE+HIPS (Asia Pacific)
Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
CTE, linear, Parallel to Flow 74.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP RFL36L PA 66
LNP* LUBRICOMP* RFL36L is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible.
CTE, linear, Parallel to Flow 74.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP RFL36L PA 66 (Asia Pacific)
LNP* Lubricomp* RFL36L is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
CTE, linear, Parallel to Flow 74.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT
LNP* LUBRICOMP* WBL36L is a compound based on PBT resin containing 30% Glass Bead, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible.
CTE, linear, Parallel to Flow 74.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT (Asia Pacific)
LNP* Lubricomp* WBL36L is a compound based on Polybutylene Terephalate resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
CTE, linear, Parallel to Flow 74.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
41.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT (Asia Pacific)
LNP* Lubricomp* WBL36L is a compound based on Polybutylene Terephalate resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
CTE, linear, Parallel to Flow 74.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Asia Pacific)
Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a..
CTE, linear, Parallel to Flow 74.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Asia Pacific)
Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a..
CTE, linear, Parallel to Flow 74.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL PVX0901 PPE+PS (Asia Pacific)
Multi purpose V1 grade
CTE, linear, Parallel to Flow 74.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Lubricomp CI001 PS (Asia Pacific)
LNP* Lubricomp* CI001 is a compound based on Polystyrene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pa..
CTE, linear, Parallel to Flow 74.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP DL003E PC
LNP LUBRICOMP* DL003E is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Easy Molding, Internally Lubricated
CTE, linear, Parallel to Flow 74.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL FP6130 PPE+PS
Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a..
CTE, linear, Parallel to Flow 74.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL FP6130 PPE+PS
Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a..
CTE, linear, Parallel to Flow 74.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Europe-Africa-Middle East)
Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a..
CTE, linear, Parallel to Flow 74.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Europe-Africa-Middle East)
Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a..
Copyright © lookpolymers.com All Rights Reserved