SABIC Innovative Plastics LNP LUBRICOMP DL003E PC

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP DL003E PC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP LUBRICOMP* DL003E is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Easy Molding, Internally Lubricated
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
ASTM D792
1.29 g/cc
0.0466 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0080 - 0.0090 cm/cm

@Time 86400 sec
0.0080 - 0.0090 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 - 0.0090 cm/cm

@Time 86400 sec
0.0080 - 0.0090 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
ISO 527
50.0 MPa
7250 psi
ASTM D638
Tensile Strength, Yield 45.0 MPa
6530 psi
ASTM D638
54.0 MPa
7830 psi
ISO 527
Elongation at Break 9.6 %
9.6 %
ISO 527
25.5 %
25.5 %
ASTM D638
Elongation at Yield 5.5 %
5.5 %
ISO 527
5.6 %
5.6 %
ASTM D638
Tensile Modulus 2.18 GPa
316 ksi
50 mm/min; ASTM D638
2.20 GPa
319 ksi
1 mm/min; ISO 527
Flexural Strength 82.0 MPa
11900 psi
ASTM D790
84.0 MPa
12200 psi
ISO 178
Flexural Modulus 2.30 GPa
334 ksi
ISO 178
2.30 GPa
334 ksi
ASTM D790
Izod Impact, Notched 1.43 J/cm
2.68 ft-lb/in
ASTM D256
Izod Impact, Unnotched 21.36 J/cm
40.02 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 16.0 kJ/m²
7.61 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 100 kJ/m²
47.6 ft-lb/in²
80*10*4; ISO 180/1U
Coefficient of Friction, Dynamic 0.18
0.18
ASTM D3702 Modified
Coefficient of Friction, Static 0.070
0.070
ASTM D3702 Modified
K (wear) Factor 121 x 10-8 mm³/N-M
60.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 73.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
74.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 75.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
75.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 138 °C
280 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 128 °C
262 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
116 °C

@Thickness 3.20 mm
241 °F

@Thickness 0.126 in
unannealed; ASTM D648