Thermal Properties Metric English Comments
Solidus 70.0 °C
158 °F
Indium Corp. Indalloy 43 Bismuth Solder Alloy
Information Provided by Indium Corporation
Solidus 70.0 °C
158 °F
Indium Corp. Indalloy 47 Bismuth-Lead-Tin Solder Alloy
Information Provided by Indium Corporation
Solidus 70.0 °C
158 °F
Indium Corp. Indalloy 65 Bismuth-Lead-Tin Solder Alloy
Information Provided by Indium Corporation
Solidus 70.0 °C
158 °F
Indium Corp. Indalloy 22 Bismuth Solder Alloy
Information Provided by Indium Corporation
Solidus 70.0 °C
158 °F
Indium Corp. Indalloy 23 Bismuth Solder Alloy
Non-electrical solder for low-ambient temperatureInformation Provided by Indium Corporation
Solidus 70.0 °C
158 °F
Indium Corp. Indalloy 24 Bismuth Solder Alloy
Information Provided by Indium Corporation
Solidus 70.0 °C
158 °F
Indium Corp. Indalloy 26 Bismuth Solder Alloy
Information Provided by Indium Corporation
Solidus 70.0 °C
158 °F
Indium Corp. Indalloy® 158 Bi-Pb-Sn-Cd Solder Alloy
Lowest melting point solder. Good fusible alloy used for lens blocking.Information provided by the manufacturer, Indium Corporation.