Indium Corp. Indalloy 23 Bismuth Solder Alloy

Category Metal , Nonferrous Metal , Bismuth Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 23 Bismuth Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non-electrical solder for low-ambient temperatureInformation Provided by Indium Corporation
Physical Properties Metric English Comments
Density 9.60 g/cc
0.347 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 25
25
Tensile Strength at Break 31.4 MPa
4550 psi
Elongation at Break 30 %
30 %
Thermal Properties Metric English Comments
Melting Point 70.0 - 73.0 °C
158 - 163 °F
Solidus 70.0 °C
158 °F
Liquidus 73.0 °C
163 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 50 %
50 %
Cadmium, Cd 12.5 %
12.5 %
Lead, Pb 25 %
25 %
Tin, Sn 12.5 %
12.5 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000550 ohm-cm
0.0000550 ohm-cm