Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 70.0 °C | 158 °F | |
Indium Corp. Indalloy 43 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 70.0 °C | 158 °F | |
Indium Corp. Indalloy 47 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 70.0 °C | 158 °F | |
Indium Corp. Indalloy 65 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 70.0 °C | 158 °F | |
Indium Corp. Indalloy 22 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 70.0 °C | 158 °F | |
Indium Corp. Indalloy 23 Bismuth Solder Alloy Non-electrical solder for low-ambient temperatureInformation Provided by Indium Corporation |
|||
Solidus | 70.0 °C | 158 °F | |
Indium Corp. Indalloy 24 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 70.0 °C | 158 °F | |
Indium Corp. Indalloy 26 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 70.0 °C | 158 °F | |
Indium Corp. Indalloy® 158 Bi-Pb-Sn-Cd Solder Alloy Lowest melting point solder. Good fusible alloy used for lens blocking.Information provided by the manufacturer, Indium Corporation. |