Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 9.32 g/cc
0.337 lb/in³
Thermal Properties Metric English Comments
Melting Point 70.0 - 102 °C
158 - 216 °F
Solidus 70.0 °C
158 °F
Liquidus 102 °C
216 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 40.5 %
40.5 %
Cadmium, Cd 9.3 %
9.3 %
Lead, Pb 27.8 %
27.8 %
Tin, Sn 22.4 %
22.4 %