Material Notes:
ZIRCAR Alumina Papers are uniform structures made principally of alumina fiber. APA-3 is a thin uniformly rigidized sheet of alumina fiber and binder. Applications include thermal insulation in low mass furnaces and thermal process systems operating to 1650°C (3002°F) high temperature gaskets and seals, separator in multifoil vacuum furnace insulation systems, expansion joint insulation, backup thermal insulation in molten metal troughs, furnaces and thermal process systems operating to high temperatures, and parting agent and barrier layer in brazing, heat-treating and metal forming processes.Information provided by Zircar Ceramics.
Physical Properties Metric English Comments
Density 0.700 g/cc
0.0253 lb/in³
at 0.06 MPa
Thickness 305 microns
12.0 mil
at 0 pressure
305 microns
12.0 mil
at 0.06 MPa
Mechanical Properties Metric English Comments
Tear Strength 1.40 kN/m
8.00 pli
Parallel to Thickness, width
Thermal Properties Metric English Comments
Thermal Conductivity 0.190 W/m-K

@Temperature 538 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 1000 °F
0.340 W/m-K

@Temperature 1370 °C
2.36 BTU-in/hr-ft²-°F

@Temperature 2500 °F
Maximum Service Temperature, Air 1650 °C
3000 °F
Component Elements Properties Metric English Comments
Al2O3 96 %
96 %
SiO2 4.0 %
4.0 %
Descriptive Properties Value Comments
Color White
Form Rigid
Type of Binder Alumina
Weight 213.4 g/m2
Users viewing this material also viewed the following: