Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 0.130 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.130 W/m-K

@Temperature 427 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 801 °F
Pyrotek I-14 Insulating Board
Pyrotek's I-14 is a low density hydrous calcium silicate board which features exceptional strength and low thermal conductivity. Inorganic and incombustible, I-14 also contains no RDF's.A..
Thermal Conductivity 0.130 W/m-K

@Temperature 800 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Pyrotek S-1100 Compressible Insulation Board
The Pyrotek S-1100 board is a low density calcium silicate product typically used for back-up insulation in refractory constructions.ApplicationsReduction cell insulation Trough covers Back-up insul..
Thermal Conductivity 0.130 - 0.230 W/m-K

@Temperature 200 °C
0.902 - 1.60 BTU-in/hr-ft²-°F

@Temperature 392 °F
Gouda Vuurvast GI 23 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.130 W/m-K

@Temperature 538 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Mid-Mountain Materials CERMEX® BK1800SW Low Biopersistence Thermal Insulation Blanket
Alkaline Earth Silicate Wool, Needled BlanketInformation provided by Mid-Mountain Materials
Thermal Conductivity 0.130 W/m-K

@Temperature 200 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 392 °F
Mean temp.; ASTM C-182
Skamol Group Moler BB-BLOCK Insulating Block
SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str..
Thermal Conductivity 0.130 W/m-K

@Temperature 200 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 392 °F
Mean temp.; ASTM C-182
Skamol Group Moler BF-BLOCK Insulating Block
SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str..
Thermal Conductivity 0.130 W/m-K

@Temperature 600 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 1110 °F
ASTM C-182
Skamol Group Moler HIPOROS Insulating Block
SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str..
Thermal Conductivity 0.130 W/m-K

@Temperature 200 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 392 °F
Mean temp.; ASTM C-182
Skamol Group V-1100 410 Vermiculite Insulating Slab
SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr..
Thermal Conductivity 0.130 W/m-K

@Temperature 200 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 392 °F
Mean temp.; ASTM C-201 supplemented by ASTM C-182
Skamol Group VERMICAST 116-25 Insulating Castable
SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f..
Thermal Conductivity 0.130 W/m-K

@Temperature 482 °C
0.900 BTU-in/hr-ft²-°F

@Temperature 900 °F
Thermal Ceramics Cease 2000 Fire
Cease Fire 2000 is a unique, two-component refractory foam. The dry powder (component A) is mixed with water to form a semi-viscous slurry and then combined with mild phosphoric acid (component B) a..
Thermal Conductivity 0.130 W/m-K

@Temperature 538 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 1000 °F
8 pcf
Thermal Ceramics Cerablanket Blanket
Cerablanket is produced from exceptionally pure oxides of alumina and silica using the spinning process. The resultant quality spun fibers have been optimized for high handling strength, with on ave..
Thermal Conductivity 0.130 W/m-K

@Temperature 538 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 1000 °F
8 pcf
Thermal Ceramics Cerachrome Blanket
Made from spun alumina-silica-chromia fiber, Cerachrome Blanket is well suited for hot face lining applications where higher temperatures are encountered, such as soaking pit covers, reheat and forg..
Thermal Conductivity 0.130 W/m-K

@Temperature 540 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Thermal Ceramics TR-19 Block Insulation
TR-19 Block is an asbestos-free insulation products, manufactured from vermiculite granules and high temperature bonding materials. Because of its low conductivity, TR-19 Block is an economical, ene..
Thermal Conductivity 0.130 W/m-K

@Temperature 538 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Thermal Ceramics V-19 Block Insulation
V-19 Block is manufactured from vermiculite granules and high-temperature bonding materials. This versatile product is available in thicknesses up to 4".V-19 Block is an economical, energy saving in..
Thermal Conductivity 0.130 W/m-K

@Temperature 760 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 1400 °F
Parallel to Thickness; ASTM C177-76
Zircar Ceramics AB Alumina Blanket
Two varieties of quilted alumina fiber blanket that have good handleability and offer very low thermal conductivity. These resilient blankets are easily cut and applied to numerous application with ..
Thermal Conductivity 0.130 W/m-K

@Temperature 800 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Parallel to Thickness; ASTM C177-76
Zircar Ceramics ALC Alumina Insulation
ALC is the same material as ZAL-15 - but brings exceptional uniformity in an insulation material in cylindrical form.Information provided by Zircar Ceramics.
Thermal Conductivity 0.130 W/m-K

@Temperature 760 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 1400 °F
Parallel to thickness; ASTM C177-76
Zircar Ceramics MB Alumina Blanket
Two varieties of quilted alumina fiber blanket that have good handleability and offer very low thermal conductivity. These resilient blankets are easily cut and applied to numerous application with ..
Thermal Conductivity 0.130 W/m-K

@Temperature 760 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 1400 °F
parallel to thickness; ASTM C177
Zircar Refractory Composites RSMAT-3000 ALUMINA MAT
ZRCI Type RSMAT-3000 is a high purity, high temperature, flexible form composed of continuous 97% alumina ceramic fibers designed for use to 1650°C (3002°F). Type RSMAT-3000 contains little shot a..
Thermal Conductivity 0.130 W/m-K

@Temperature 760 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 1400 °F
Parallel to Thickness; ASTM C177-76
Zircar Ceramics Alumina Mat
A layered, low density flexible mat made of 100% polycrystalline alumina fiber (non-RCF) designed for use to temperatures as high as 1650°C (3002°F). Shot free low density mat used as fill between..
Thermal Conductivity 0.130 W/m-K

@Temperature 871 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 1600 °F
Zircar Refractory Composites ASPA-2 Alumina-Silica Fiber Paper
ASPA-2 is a premium grade, lightweight refractory material made from high purity alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal c..
Thermal Conductivity 0.130 W/m-K

@Temperature 100 °C
0.900 BTU-in/hr-ft²-°F

@Temperature 212 °F
ChevronTexaco 22 Heat Transfer Oil
FeaturesChevron Heat Transfer Oils are mineral-type transfer oils for use in secondary or indirect heating systems. They are formulated with ISOSYN® base stocks. Chevron Heat Transfer Oils are nont..
Thermal Conductivity 0.130 W/m-K

@Temperature 204 °C
0.900 BTU-in/hr-ft²-°F

@Temperature 400 °F
Duratherm 450 Paraffinic Heat Transfer Fluid
Duratherm 450 - thermal fluid specifically engineered for applications requiring process heating and cooling efficiently between 30°F and 450°F. Economical and thermally stable, Duratherm 450 offe..
Thermal Conductivity 0.130 W/m-K

@Temperature 260 °C
0.900 BTU-in/hr-ft²-°F

@Temperature 500 °F
Duratherm 600 Paraffinic Heat Transfer Fluid
Duratherm 600 - thermal fluid rated to 600°F it contains the industries most aggressive blend of additives for long, trouble free operation in a variety of applications. Specifically engineered to ..
Thermal Conductivity 0.130 W/m-K

@Temperature 288 °C
0.900 BTU-in/hr-ft²-°F

@Temperature 550 °F
Duratherm FG Paraffinic Heat Transfer Fluid
Duratherm FG - thermal oil rated to 620°F it is engineered and manufactured to comply with the demands of food grade applications. NSF registered, meets USDA requirements for incidental food contac..
Thermal Conductivity 0.130 W/m-K

@Temperature 37.8 °C
0.900 BTU-in/hr-ft²-°F

@Temperature 100 °F
Duratherm S Silicone Heat Transfer Fluid
Duratherm S - a silicone based heat transfer fluid that is ideally suited for high oxidation or completely exposed systems up to 650°F. Duratherm S is virtually impervious to oxidation and offers s..
Thermal Conductivity 0.130 W/m-K

@Temperature 260 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 500 °F
ASTM C182
BNZ Materials BNZ-23A Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.130 W/m-K

@Temperature 260 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 500 °F
ASTM C182
BNZ Materials BNZ-24 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.130 W/m-K

@Temperature 482 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 900 °F
Thermal Ceramics Kaomat 200-SL Blanket
Kaomat 2000-SL silica blanket is a high temperature "shot free" amorphous silica blanket which has been heat treated during the manufacturing process to reduce residual shrinkage. This durable produ..
Thermal Conductivity 0.130 W/m-K

@Temperature 600 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Zircar Ceramics ECO-27B Alumina-Silica Insulation
This utility grade board is produced with or without organic binder. Useful to temperatures of 1260°C (2300°F) ECO-27 offers exceptional strength and durability. Information provided by Zircar Cer..
Thermal Conductivity 0.130 W/m-K

@Temperature 316 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 601 °F
3M Nextel™ AF-14 Industrial Woven Fabric 312