Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.130 - 0.230 W/m-K @Temperature 200 °C |
0.902 - 1.60 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Gouda Vuurvast GI 23 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |