Material Notes:
The Pyrotek S-1100 board is a low density calcium silicate product typically used for back-up insulation in refractory constructions.ApplicationsReduction cell insulation Trough covers Back-up insulation AdvantagesExceptional heat resistance Low thermal conductivity High mechanical strength Not damaged by water Excellent creep resistance Dimensional stability Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 0.250 g/cc
0.00903 lb/in³
Mechanical Properties Metric English Comments
Flexural Strength 1.40 MPa
203 psi
Compressive Strength 2.50 MPa
363 psi
Thermal Properties Metric English Comments
Thermal Conductivity 0.0440 W/m-K

@Temperature 20.0 °C
0.305 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
0.0810 W/m-K

@Temperature 400 °C
0.562 BTU-in/hr-ft²-°F

@Temperature 752 °F
0.130 W/m-K

@Temperature 800 °C
0.902 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Maximum Service Temperature, Air 1100.5 °C
2012.9 °F
Component Elements Properties Metric English Comments
Al2O3 0.30 %
0.30 %
CaO 44.9 %
44.9 %
Fe2O3 0.30 %
0.30 %
K2O 0.10 %
0.10 %
MgO 0.60 %
0.60 %
Na2O 0.10 %
0.10 %
SiO2 47.5 %
47.5 %
Processing Properties Metric English Comments
Moisture Content 5.5 %
5.5 %