Thermal Properties Metric English Comments
Vicat Softening Point 104 °C

@Thickness 4.00 mm
219 °F

@Thickness 0.157 in
Rate A; ISO 306/A50
Premix Thermoplastics PRE-ELEC® ABS 1410
PRE-ELEC ABS 1410 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ABS 141..
Vicat Softening Point 104 °C

@Load 1.00 kg
219 °F

@Load 2.20 lb
120°C/min; ASTM D1525
Kingfa H-12 Modified ABS
Features:UL94 HB @ 1.6-3.0mmHigh toughnessHeat resistanceApplications:Automobile exterior trimAutomobile interior trimPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Vicat Softening Point 104 °C

@Load 1.00 kg
219 °F

@Load 2.20 lb
120°C/hour; ISO 306
Ineos ABS Lustran® 288 ABS, Injection Molding Grade
Lustran® ABS 288 is a very high-flow injection molding grade of ABS (acrylonitrile butadiene styrene) with good impact strength and high gloss. It is intended for use in a wide range of applicati..
Vicat Softening Point 104 °C

@Load 1.02 kg
219 °F

@Load 2.25 lb
50°C/h; ISO 306
Styrolution Terluran® HI-12 ABS
Terluran HI-12 is an injection molding grade of ABS with a very high toughness and easy flow.Very high toughnessEasy flowingUL 94 HB (1.6 & 3.2 mm)Information provided by Styrolution
Vicat Softening Point 104 °C

@Load 0.999 kg
219 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 1016 V0 Flame Retardant ABS
Acrylonitrile Butadiene StyreneFlame retardant class V0, with PBDE, good physical and mechanical characteristics, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 104 °C

@Load 0.999 kg
219 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 1218 V0 Flame Retardant ABS
Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, good impact resistance, excellent processability, good surface appearance, good thermal resistanceInformation provided by Cossa Po..
Vicat Softening Point 104 °C

@Load 0.999 kg
219 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE CR 1 Acrylonitrile Butadiene Styrene
ABS for chrome platingGood melt flow rate, high impact resistance at low temperature, high gloss, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 104 °C

@Load 5.10 kg
219 °F

@Load 11.2 lb
120°C/h; ISO 306
Covestro Bayblend® FR3005 HG PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
Vicat Softening Point 104 °C

@Load 5.00 kg
219 °F

@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Kibisan® PN-117 SAN
Injection Molding
Vicat Softening Point 104 °C

@Load 5.00 kg
219 °F

@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Kibisan® PN-117C SAN
High Clarity
Vicat Softening Point 104 °C

@Load 5.00 kg
219 °F

@Load 11.0 lb
50°C/hr; ISO 306
Chi Mei Kibisan® PN-127 SAN
Heat Resistant
Vicat Softening Point 104 °C

@Load 5.00 kg
219 °F

@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Kibisan® PN-127 SAN
Heat Resistant
Vicat Softening Point 104 °C

@Load 1.00 kg
219 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-709 ABS
Super impact
Vicat Softening Point 104 °C

@Load 1.00 kg
219 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-709S ABS - Extrusion
Super Impact Extrusion
Vicat Softening Point 104 °C

@Load 1.00 kg
219 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-716 ABS - High Flow
High flow, medium impact
Vicat Softening Point 104 °C

@Load 5.00 kg
219 °F

@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-747R ABS - Extrusion
Attach case and refrigerator
Vicat Softening Point 104 °C

@Load 1.00 kg
219 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Polyrex® PH-60 Polystyrene - High Impact
Medium impact
Vicat Softening Point 104 °C

@Load 1.00 kg
219 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Polyrex® PH-88S Polystyrene - Extrusion
Extrusion
Vicat Softening Point 104 °C

@Load 5.00 kg
219 °F

@Load 11.0 lb
50°C/hr; ISO 306
Chi Mei Kibisan® PN-127H SAN
Chemical Resistant
Vicat Softening Point 104 °C

@Load 5.00 kg
219 °F

@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Kibisan® PN-127H SAN
Chemical Resistant
Vicat Softening Point 104 °C

@Load 1.00 kg
219 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-707 ABS
High gloss, high rigid
Vicat Softening Point 104 °C

@Load 1.00 kg
219 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-746H ABS - High Flow
Super high flow, medium impact
Vicat Softening Point 104 °C

@Load 1.00 kg
219 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-756 ABS - High Flow
High rigid, high flow
Vicat Softening Point 104 °C

@Load 1.00 kg
219 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-756H ABS - High Flow
Super high flow
Vicat Softening Point 104 °C

@Load 1.00 kg
219 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-756S ABS - High Flow
Super high flow, medium impact
Vicat Softening Point 104 °C

@Load 1.00 kg
219 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-757 ABS
High gloss, medium impact
Vicat Softening Point 104 °C

@Load 1.00 kg
219 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-758 ABS - Transparent
Transparent
Vicat Softening Point 104 °C

@Load 1.00 kg
219 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-763 ABS - Flame Retardant
F.R. High Heat Weather Resistant
Vicat Softening Point 104 °C

@Load 1.00 kg
219 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-763A ABS - Flame Retardant
F.R. High Heat
Vicat Softening Point 104 °C

@Load 1.00 kg
219 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-746Y ABS  (discontinued **)
Medium flow, high impact