Thermal Properties Metric English Comments
Maximum Service Temperature, Air 86.0 °C
187 °F
Deflection temperature; load unknown.
Abatron AboCast 8-14/Abocure 8-14 Epoxy  (discontinued **)
2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/12.10 ratio (pbw); Gel time, 100 g (3.5 oz.): 63 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°..
Maximum Service Temperature, Air 86.0 °C
187 °F
Deflection temperature; load unknown.
Abatron AboCast 8-16/Abocure 8-16 Epoxy  (discontinued **)
2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/35.00 ratio (pbw); Gel time, 100 g (3.5 oz.): 57 minutes; cures in 2 weeks at 25°C (77°F).Applications: solventless ca..
Maximum Service Temperature, Air 86.0 - 96.0 °C
187 - 205 °F
Softening Range
Huntsman Araldite GT 7014 Bisphenol A Epoxy Solid Resin
Weight per Epoxide (EEW, g/eq) 725 to 775. Max color is 1.Comments/Applications: Unmodified bis A "Type 3+" epoxy. Medium flow resin especially designed for powder coatings.Data provided by Ciba S..
Maximum Service Temperature, Air 86.0 - 96.0 °C
187 - 205 °F
Softening Range
Huntsman Araldite GT 9014 US Bisphenol A Epoxy Solid Resin
Weight per Epoxide (EEW, g/eq) 700 to 760. Max color is 1.Comments/Applications: Unmodified bis A "Type 3 1/2" epoxy resin. Slightly higher molecular weight than GT 7013 leads to improved mixing a..
Maximum Service Temperature, Air 86.0 °C
187 °F
Heat deflection temperature, load unknown; ASTM D648
LG Chemical AT-553 Transparent ABS, Permanent Antistatic, Natural and Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
Maximum Service Temperature, Air 86.0 °C
187 °F
Heat Distortion Temp
Lucky IF-870 Acrylic, High Flow Grade
High flow for thin-walled injection molded parts and parts with long flow paths. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistanc..
Maximum Service Temperature, Air 86.0 °C
187 °F
Deflection Temp; Load not reported; ASTM D648
Lucky IF-870 Acrylic, High Flow Grade
High flow for thin-walled injection molded parts and parts with long flow paths. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistanc..