Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucky IF-870 Acrylic, High Flow Grade

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, General Purpose, Molded
Manufacturer Lucky
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucky IF-870 Acrylic, High Flow Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High flow for thin-walled injection molded parts and parts with long flow paths. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring capability.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D955-51
Melt Flow 23 g/10 min
23 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 84
84
ASTM D785
Tensile Strength, Ultimate 65.0 MPa
9430 psi
ASTM D638
Elongation at Break 2.5 %
2.5 %
ASTM D638
Flexural Yield Strength 90.0 MPa
13100 psi
ASTM D790
Flexural Modulus 3.20 GPa
464 ksi
ASTM D790
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 86.0 °C
187 °F
Heat Distortion Temp
86.0 °C
187 °F
Deflection Temp; Load not reported; ASTM D648
Vicat Softening Point 85.0 °C
185 °F
ASTM D1525
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.17 mm
HB

@Thickness 0.125 in
Optical Properties Metric English Comments
Refractive Index 1.49
1.49
ASTM D542
Transmission, Visible 92 %
92 %
ASTM D1003
Electrical Properties Metric English Comments
Dielectric Strength 20.0 kV/mm
508 kV/in
ASTM D149
Copyright © lookpolymers.com All Rights Reserved