Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 86.0 - 96.0 °C | 187 - 205 °F | Softening Range |
Huntsman Araldite GT 7014 Bisphenol A Epoxy Solid Resin Weight per Epoxide (EEW, g/eq) 725 to 775. Max color is 1.Comments/Applications: Unmodified bis A "Type 3+" epoxy. Medium flow resin especially designed for powder coatings.Data provided by Ciba S.. |
|||
Maximum Service Temperature, Air | 86.0 - 96.0 °C | 187 - 205 °F | Softening Range |
Huntsman Araldite GT 9014 US Bisphenol A Epoxy Solid Resin Weight per Epoxide (EEW, g/eq) 700 to 760. Max color is 1.Comments/Applications: Unmodified bis A "Type 3 1/2" epoxy resin. Slightly higher molecular weight than GT 7013 leads to improved mixing a.. |
|||
Maximum Service Temperature, Air | 90.0 - 96.0 °C | 194 - 205 °F | Softening point |
Mitsui MILEXâ„¢ XL-325M Phenol Aralkyl Resin, High Molecular Weight The MILEXâ„¢ Family of products is widely featured in brake systems of automobiles made by automakers through Mitsui Chemicals'. The phenolic material is primarily used as binders in brake pad.. |