Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 86.0 °C | 187 °F | Deflection temperature; load unknown. |
Abatron AboCast 8-14/Abocure 8-14 Epoxy
(discontinued **) 2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/12.10 ratio (pbw); Gel time, 100 g (3.5 oz.): 63 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°.. |
|||
Maximum Service Temperature, Air | 86.0 °C | 187 °F | Deflection temperature; load unknown. |
Abatron AboCast 8-16/Abocure 8-16 Epoxy
(discontinued **) 2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/35.00 ratio (pbw); Gel time, 100 g (3.5 oz.): 57 minutes; cures in 2 weeks at 25°C (77°F).Applications: solventless ca.. |
|||
Maximum Service Temperature, Air | 86.0 - 96.0 °C | 187 - 205 °F | Softening Range |
Huntsman Araldite GT 7014 Bisphenol A Epoxy Solid Resin Weight per Epoxide (EEW, g/eq) 725 to 775. Max color is 1.Comments/Applications: Unmodified bis A "Type 3+" epoxy. Medium flow resin especially designed for powder coatings.Data provided by Ciba S.. |
|||
Maximum Service Temperature, Air | 86.0 - 96.0 °C | 187 - 205 °F | Softening Range |
Huntsman Araldite GT 9014 US Bisphenol A Epoxy Solid Resin Weight per Epoxide (EEW, g/eq) 700 to 760. Max color is 1.Comments/Applications: Unmodified bis A "Type 3 1/2" epoxy resin. Slightly higher molecular weight than GT 7013 leads to improved mixing a.. |
|||
Maximum Service Temperature, Air | 86.0 °C | 187 °F | Heat deflection temperature, load unknown; ASTM D648 |
LG Chemical AT-553 Transparent ABS, Permanent Antistatic, Natural and Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Maximum Service Temperature, Air | 86.0 °C | 187 °F | Heat Distortion Temp |
Lucky IF-870 Acrylic, High Flow Grade High flow for thin-walled injection molded parts and parts with long flow paths. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistanc.. |
|||
Maximum Service Temperature, Air | 86.0 °C | 187 °F | Deflection Temp; Load not reported; ASTM D648 |
Lucky IF-870 Acrylic, High Flow Grade High flow for thin-walled injection molded parts and parts with long flow paths. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistanc.. |