Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Styrolution Clearblend 165 MBS

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Styrolution
Trade Name Clearblend
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styrolution Clearblend 165 MBS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CLEARBLEND 165 is an impact modified styrene acrylic copolymer blend with excellent clarity and outstanding toughness.Exceptional toughnessLow densityEase of processingLow moisture absorptionInformation provided by Styrolution
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D 792
Water Absorption at Saturation 0.10 %

@Temperature 23.0 °C
0.10 %

@Temperature 73.4 °F
ASTM D 570
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D 955
Melt Flow 5.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell M 70
70
ASTM D 785
Tensile Strength, Yield 20.7 MPa
3000 psi
ASTM D 638
Elongation at Break 50 %
50 %
ASTM D 638
Tensile Modulus 1.52 GPa
220 ksi
ASTM D 638
Flexural Strength 37.2 MPa
5400 psi
ASTM D 790
Flexural Modulus 1.55 GPa
225 ksi
ASTM D 790
Izod Impact, Notched 2.67 J/cm
5.00 ft-lb/in
ASTM D 256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 249 °C
480 °F
Vicat Softening Point 93.9 °C
201 °F
ASTM D 1525
Optical Properties Metric English Comments
Refractive Index 1.57
1.57
Sodium D Line; ASTM D 542
Haze 2.2 %
2.2 %
ASTM D 1003
Transmission, Visible >= 90 %

@Wavelength 550 nm
>= 90 %

@Wavelength 550 nm
ASTM D 1003
Processing Properties Metric English Comments
Melt Temperature 204 - 238 °C
400 - 460 °F
Mold Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Drying Temperature 65.6 °C

@Time 7200 sec
150 °F

@Time 2.00 hour