Styrolution Clearblend 145 MBS

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Styrolution
Trade Name Clearblend
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styrolution Clearblend 145 MBS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Clearblend 145 is an impact modified styrene acrylic copolymer blend with excellent clarity.Excellent clarityLow densityEase of processingLow moisture absorptionInformation provided by Styrolution
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D 792
Water Absorption at Saturation 0.10 %

@Temperature 23.0 °C
0.10 %

@Temperature 73.4 °F
ASTM D 570
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D 955
Melt Flow 3.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell M 80
80
ASTM D 785
Tensile Strength, Yield 27.6 MPa
4000 psi
ASTM D 638
Elongation at Break 40 %
40 %
ASTM D 638
Tensile Modulus 2.24 GPa
325 ksi
ASTM D 638
Flexural Strength 55.2 MPa
8000 psi
ASTM D 790
Flexural Modulus 2.28 GPa
330 ksi
ASTM D 790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D 256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 249 °C
480 °F
Vicat Softening Point 97.8 °C
208 °F
ASTM D 1525
Optical Properties Metric English Comments
Refractive Index 1.57
1.57
Sodium D Line; ASTM D 542
Haze 2.0 %
2.0 %
ASTM D 1003
Transmission, Visible >= 90 %

@Wavelength 550 nm
>= 90 %

@Wavelength 550 nm
ASTM D 1003
Processing Properties Metric English Comments
Melt Temperature 204 - 238 °C
400 - 460 °F
Mold Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Drying Temperature 65.6 °C

@Time 7200 sec
150 °F

@Time 2.00 hour